Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 1586 Polyester, Pellet, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass and Mineral Filled BMC
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 1586 Polyester, Pellet, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injection molded electrical appliance components. UL recognized under component file E40654. 01586 is available in white.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.890 g/cc
0.0322 lb/in³
ASTM D1895
Density 1.89 g/cc
0.0683 lb/in³
ASTM D792
Water Absorption 0.059 %
0.059 %
ASTM D570
Linear Mold Shrinkage 0.0037 cm/cm
0.0037 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 54
54
ASTM D785
Tensile Strength, Ultimate 64.0 MPa
9280 psi
ASTM D638
Elongation at Break 1.09 %
1.09 %
ASTM D638
Tensile Modulus 11.7 GPa
1700 ksi
ASTM D638
Flexural Strength 101 MPa
14600 psi
ASTM D790
Flexural Modulus 10.2 GPa
1480 ksi
ASTM D790
Compressive Strength 119 MPa
17300 psi
ASTM D695
Poissons Ratio 0.32
0.32
ASTM D638
Shear Modulus 4.43 GPa
643 ksi
Calculated
Izod Impact, Notched 0.410 J/cm
0.768 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
ASTM D256
Impact 289
289
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 86.0 µm/m-°C

@Temperature 40.0 - 130 °C
47.8 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.870 W/m-K

@Temperature 100 °C
6.04 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 217 °C
423 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
486 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.00 mm
V-0

@Thickness 0.0394 in
Oxygen Index 41 %
41 %
ASTM D2863
Shrinkage 0.0072 %
0.0072 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.80e+15 ohm-cm
1.80e+15 ohm-cm
ASTM D247
Dielectric Constant 4.4
4.4
ASTM D150
Dielectric Strength 11.1 kV/mm
282 kV/in
Step by Step; ASTM D149
13.0 kV/mm
330 kV/in
Short Time; ASTM D149
Dielectric Breakdown 23000 V
23000 V
1hr 120C; ASTM D149
Dissipation Factor 0.0173
0.0173
ASTM D150
Arc Resistance 189 sec
189 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638