Plenco 1510 Polyester, Pellet, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 1510 Polyester, Pellet, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file E40654. 01510 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.960 g/cc
0.0347 lb/in³
ASTM D1895
Density 2.02 g/cc
0.0730 lb/in³
ASTM D792
Water Absorption 0.126 %
0.126 %
ASTM D570
Linear Mold Shrinkage 0.0038 cm/cm
0.0038 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 72
72
ASTM D785
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ASTM D638
Elongation at Break 0.51 %
0.51 %
ASTM D638
Tensile Modulus 21.3 GPa
3090 ksi
ASTM D638
Flexural Strength 114 MPa
16500 psi
ASTM D790
Flexural Modulus 19.1 GPa
2770 ksi
ASTM D790
Compressive Strength 155 MPa
22500 psi
ASTM D695
Izod Impact, Notched 0.220 J/cm
0.412 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.227 J/cm²
1.08 ft-lb/in²
ASTM D256
Impact 126
126
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 48.0 µm/m-°C

@Temperature 40.0 - 130 °C
26.7 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 215 °C
419 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 249 °C
480 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 24.5 %
24.5 %
ASTM D2863
Shrinkage 0.00182 %
0.00182 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 3.70e+15 ohm-cm
3.70e+15 ohm-cm
ASTM D247
Dielectric Constant 4.6
4.6
ASTM D150
Dielectric Strength 11.5 kV/mm
292 kV/in
Step by Step; ASTM D149
15.3 kV/mm
389 kV/in
Short Time; ASTM D149
Dielectric Breakdown 23000 V
23000 V
1hr 120C; ASTM D149
Dissipation Factor 0.0153
0.0153
ASTM D150
Arc Resistance 191 sec
191 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638