Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 55 - 65 dB @Thickness 3.00 mm |
55 - 65 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific) LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically
Conductive, EMI/RFI Shielding.This data was suppli.. |