Material Notes:
P & P Technology SP, SS, SR, SW & SF Ranges of gasket materials consist of Monel or aluminum wires embedded into solid silicone, sponge silicone or fluorosilicone, a fire retardant variant is also available. The material may be supplied in strip form or as a complete gasket with or without pressure sensitive adhesive tape. Other options include compression stops or collars. Carrier: SP Solid Silicone Elastomer (Grey) to ZZ-R-765 2b 40 SS Sponge Silicone (Grey) AMS3195 to ZZ-R-765-2b-40 SR Solid Silicone Fire Retardant (Black) to ZZ-R-765 *SF Fluorosilicone (Blue) to Mil-R-25988 Gr5 SG Sponge Silicone Fire Retardant (Black) to AMS3195 Wire:Monel 0.11mm dia. to QQ-N-281 Aluminuma dia. 0.12 mm Alloy 5056 Self adhesive: Pressure sensitive adhesive (if specified) Release liner: White siliconised paperAdhesive type: Modified acrylic Compression: Maximum Recommended 20% Wire Count:100 ± 15% per cm2(solid) 80 ± 15% per cm2(sponge)Information provided by P & P Technology
Physical Properties Metric English Comments
Thickness 70.0 microns
2.76 mil
Mechanical Properties Metric English Comments
Hardness, Shore A 30 - 40
30 - 40
Elastomer, Solid, Micro
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Electrical Properties Metric English Comments
Shielding Effectiveness 55 dB

@Frequency 10000 Hz
55 dB

@Frequency 10000 Hz
H-Field
60 dB

@Frequency 1.00e+10 Hz
60 dB

@Frequency 1.00e+10 Hz
P-Field
83 dB

@Frequency 100000 Hz
83 dB

@Frequency 100000 Hz
H-Field
95 dB

@Frequency 1.00e+9 Hz
95 dB

@Frequency 1.00e+9 Hz
P-Field
>= 102 dB

@Frequency 1.00e+6 Hz
>= 102 dB

@Frequency 1.00e+6 Hz
H-Field
>= 102 dB

@Frequency 4.00e+8 Hz
>= 102 dB

@Frequency 4.00e+8 Hz
P-Field
>= 120 dB

@Frequency 1.00e+7 Hz
>= 120 dB

@Frequency 1.00e+7 Hz
E-Field
>= 121 dB

@Frequency 1.00e+7 Hz
>= 121 dB

@Frequency 1.00e+7 Hz
E-Field
>= 140 dB

@Frequency 1.00e+8 Hz
>= 140 dB

@Frequency 1.00e+8 Hz
E-Field
>= 141 dB

@Frequency 1.00e+6 Hz
>= 141 dB

@Frequency 1.00e+6 Hz
E-Field
Descriptive Properties Value Comments
Adhesion Aged 31N/25mm
Adhesion Initial 31N/25mm