PolyOne LubriOne™ NN-30GF/10T WHT Polyamide 66 (Nylon 66)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer PolyOne Corporation
Trade Name LubriOne™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne LubriOne™ NN-30GF/10T WHT Polyamide 66 (Nylon 66).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. LubriOne compounds have been demonstrated to reduce friction, noise, vibration, heat buildup and improve product durability.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Water Absorption 0.50 %

@Temperature 23.0 °C
0.50 %

@Temperature 73.4 °F
@ 24 hrs; Internal Method
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 82

@Temperature 23.0 °C
82

@Temperature 73.4 °F
15 sec; ASTM D2240
83

@Temperature 23.0 °C
83

@Temperature 73.4 °F
ASTM D2240
Tensile Strength 172 MPa
24900 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 9.65 GPa
1400 ksi
ASTM D638
Flexural Strength 241 MPa
35000 psi
ASTM D790
Flexural Modulus 9.65 GPa
1400 ksi
ASTM D790
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 244 °C
471 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Dielectric Strength 8.50 kV/mm

@Temperature 23.0 °C
216 kV/in

@Temperature 73.4 °F
Method A (Short-Time); ASTM D149
Processing Properties Metric English Comments
Melt Temperature 288 - 299 °C
550 - 570 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Drying Temperature 71.1 - 82.2 °C
160 - 180 °F
Descriptive Properties Value Comments
Additive Lubricant
Appearance White
Features Lubricated
Forms Pellets
Generic Material Nylon 66
Generic Name Polyamide 66 (Nylon 66)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Appliance Components
Automotive Applications
Bearings
Business Equipment
Consumer Applications
Conveyor Parts
Gears
Industrial Applications
Printer Parts
Pulleys
Rollers