Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 316 - 343 °C
600 - 650 °F
Polymer Resources PC-BR1-UV Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilized
Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilizedFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical..
Melt Temperature 316 - 343 °C
600 - 650 °F
Polymer Resources PC-GP3-TFE10 Polycarbonate, 10% PTFE, High Flow, Wear Resistant
Polycarbonate, General Purpose, High Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4001 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Melt Temperature 307 - 343 °C
585 - 650 °F
RTP Company RTP 4004 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4005 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4008 A FR (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4011 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4085 A TFE 15 (Hot Water Moldable) Polyphthalamide (PPA), Carbon Fiber - PTFE Lubricated
Melt Temperature 329 - 343 °C
625 - 650 °F
RTP Company RTP 4087 A FR (Hot Water Moldable) Polyphthalamide (PPA), Carbon Fiber - Flame Retardant
Melt Temperature 310 - 343 °C
590 - 650 °F
RTP Company RTP 4400 High Temperature Nylon (HTN), Unfilled
Melt Temperature 310 - 343 °C
590 - 650 °F
RTP Company RTP 4408 L High Temperature Nylon (HTN), Glass Fiber - Lubricated
Melt Temperature 310 - 343 °C
590 - 650 °F
RTP Company RTP 4481 High Temperature Nylon (HTN), Carbon Fiber
Melt Temperature 310 - 343 °C
590 - 650 °F
RTP Company RTP 4485 High Temperature Nylon (HTN), Carbon Fiber
Melt Temperature 316 - 343 °C
600 - 650 °F
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized
Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Melt Temperature 241 - 343 °C
465 - 650 °F
Average value: 282 °C Grade Count:29
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..
Melt Temperature 249 - 343 °C
480 - 650 °F
Average value: 293 °C Grade Count:8
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..
Melt Temperature 293 - 343 °C
560 - 650 °F
Average value: 318 °C Grade Count:5
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum..
Melt Temperature 300 - 343 °C
572 - 650 °F
Average value: 320 °C Grade Count:24
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be..
Melt Temperature 316 - 343 °C
600 - 650 °F
Molding
PolyOne Edgetek® SF-20GF/000 Polyphenylene Sulfide (PPS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 316 - 343 °C
600 - 650 °F
Star Plastics PC733R Molding Grade PC
Information provided by Star Plastics, Inc.
Melt Temperature 316 - 343 °C
600 - 650 °F
Star Plastics PCGF10 Molding Grade PC with 10% Glass
Information provided by Star Plastics, Inc.
Melt Temperature 316 - 343 °C
600 - 650 °F
Star Plastics PCGF20 Molding Grade PC with 20% Glass
Information provided by Star Plastics, Inc.
Melt Temperature 316 - 343 °C
600 - 650 °F
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Melt Temperature 293 - 343 °C
560 - 650 °F
RTP Company ESD 3281 Ethylene Tetrafluoroethylene (ETFE) Carbon Fiber - Static Dissipative
Melt Temperature 293 - 343 °C
560 - 650 °F
RTP Company ESD 3282 Ethylene Tetrafluoroethylene (ETFE) Carbon Fiber - Electrically Conductive
Melt Temperature 302 - 343 °C
575 - 650 °F
RTP Company RTP 1300 D AR 15 TFE 15 Polyphenylene Sulfide (PPS), Aramid Fiber - PTFE Lubricated
Melt Temperature 302 - 343 °C
575 - 650 °F
RTP Company RTP 1378 CL Polyphenylene Sulfide (PPS), Glass Fiber Reinforced - PTFE Lubricated
Melt Temperature 310 - 343 °C
590 - 650 °F
RTP Company RTP 4405 FR L High Temperature Nylon (HTN), Glass Fiber - Flame Retardant - Lubricated
Melt Temperature 316 - 343 °C
600 - 650 °F
Molding
PolyOne Lubri-Tech™ AM-30CF/15T Polyphthalamide (PPA), Carbon Fiber Reinforced, PTFE Lubricated  (discontinued
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 293 - 343 °C
560 - 650 °F
RTP Company RTP 3299 X 120869 A NAT/BLK Ethylene Tetrafluoroethylene (ETFE), Carbon Fiber
Copyright © lookpolymers.com All Rights Reserved