NOVA Chemicals Sclair® 2909 HDPE Injection Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer NOVA Chemicals
Trade Name Sclair®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 2909 HDPE Injection Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High stiffness, Maximum impact strength and toughness, Good top loading capability, High surface glossApplications: Tote boxes, Beverage cratesAdditives: Antioxidant, Ultraviolet light stabilizersInformation provided by NOVA Chemicals.
Physical Properties Metric English Comments
Density 0.962 g/cc
0.0348 lb/in³
ASTM D792
Environmental Stress Crack Resistance <= 10 hour
<= 10 hour
F<sub>50</sub>; Condition A, 100% Igepal; ASTM D1693
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Spiral Flow 23.0 cm
9.06 in
NOVA Snake Flow Test
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 29.0 MPa
4210 psi
50 mm/min; ASTM D638
Elongation at Break 800 %
800 %
50 mm/min; ASTM D638
Flexural Modulus 1.28 GPa
186 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 129 °C
264 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 170 - 215 °C
338 - 419 °F