Material Notes:
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance range.Impact resistance.Body and duty parts in office equipment, gear wheels, grippers, sleeves, sliding elements, switches and plugs.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ISO 1183
Water Absorption <= 0.20 %
<= 0.20 %
23°C/24h
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
Melt Flow 11.16 g/10 min

@Load 1.20 kg,
Temperature 300 °C
11.16 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Mechanical Properties Metric English Comments
Tensile Stress 50.0 MPa
7250 psi
Elongation at Yield 5.0 %
5.0 %
6.0 %
6.0 %
flexural
Modulus of Elasticity 2.20 GPa
319 ksi
Flexural Strength 80.0 MPa
11600 psi
Flexural Modulus 1.80 GPa
261 ksi
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
flatwise; ISO 179 1fU
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
150 °C
302 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
Vicat Softening Point 160 °C
320 °F
DIN ISO 306
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 295 °C
563 °F
mass temp
Nozzle Temperature 290 - 310 °C
554 - 590 °F
Zone 1 280 - 300 °C
536 - 572 °F
Zone 2 290 - 310 °C
554 - 590 °F
Zone 3 300 - 320 °C
572 - 608 °F
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Drying Temperature 120 °C

@Time 14400 - 21600 sec
248 °F

@Time 4.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color white