Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® NY-4/PL/15/BK Polyamide 612, with PTFE

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® NY-4/PL/15/BK Polyamide 612, with PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Bearings, sleeves, sliding elements, control disks, gear wheels, duty parts in switches.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ISO 1183
Water Absorption <= 0.35 %
<= 0.35 %
23°C/24h
Linear Mold Shrinkage 0.014 - 0.020 cm/cm
0.014 - 0.020 in/in
Mechanical Properties Metric English Comments
Tensile Stress 45.0 MPa
6530 psi
Elongation at Yield 4.0 %
4.0 %
6.5 %
6.5 %
flexural
Flexural Strength 70.0 MPa
10200 psi
Flexural Modulus 2.00 GPa
290 ksi
Charpy Impact Unnotched 2.90 J/cm²
13.8 ft-lb/in²
flatwise; ISO 179 1fU
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179 1eA
Coefficient of Friction, Dynamic 0.27
0.27
Coefficient of Friction, Static 0.21
0.21
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 280 °C
536 °F
mass temp
Nozzle Temperature 230 - 285 °C
446 - 545 °F
Zone 1 220 - 260 °C
428 - 500 °F
Zone 2 225 - 265 °C
437 - 509 °F
Zone 3 230 - 275 °C
446 - 527 °F
Mold Temperature 60.0 - 120 °C
140 - 248 °F
Drying Temperature 80.0 °C

@Time 14400 - 21600 sec
176 °F

@Time 4.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color black