Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Elastocon TPE Technologies Elastocon® 8138B Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Elastocon TPE Technologies
Trade Name Elastocon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastocon TPE Technologies Elastocon® 8138B Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elastocon® 8138B is a black thermoplastic elastomer compound formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8138B is well suited for consumer goods and industrial applications requiring U.V. stability. Elastocon® 8138B can be overmolded to polypropylene.Information provided by Elastocon TPE Technologies, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.013 - 0.023 cm/cm
0.013 - 0.023 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 35
35
ASTM D2240
Tensile Strength 2.70 MPa
392 psi
ASTM D412
Elongation at Break 379 %
379 %
ASTM D412
100% Modulus 0.00110 GPa
0.160 ksi
ASTM D412
Compression Set 13 %

@Temperature 20.0 °C,
Time 79200 sec
13 %

@Temperature 68.0 °F,
Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Feed Temperature <= 79.4 °C
<= 175 °F
Rear Barrel Temperature 143 - 160 °C
290 - 320 °F
Front Barrel Temperature 160 - 182 °C
320 - 360 °F
Nozzle Temperature 188 - 204 °C
370 - 400 °F
Mold Temperature 21.1 - 37.8 °C
70.0 - 100 °F
Back Pressure 0.345 - 0.689 MPa
50.0 - 100 psi
Descriptive Properties Value Comments
Injection Rate Fast