Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 185 - 200 °C | 365 - 392 °F | |
Multibase TPSiV® 4100-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr.. |
|||
Nozzle Temperature | 185 - 200 °C | 365 - 392 °F | |
Multibase TPSiV® 4200-60A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Nozzle Temperature | 185 - 200 °C | 365 - 392 °F | |
Multibase TPSiV® 4200-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Nozzle Temperature | 185 - 200 °C | 365 - 392 °F | |
Multibase TPSiV® 4200-80A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Nozzle Temperature | 185 °C | 365 °F | |
Termopol Termoton® K2GA3060A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Nozzle Temperature | 185 °C | 365 °F | |
Termopol Termoton® K2GA4065A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Nozzle Temperature | 185 °C | 365 °F | |
Termopol Termoton® K4GA4070A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Nozzle Temperature | 185 °C | 365 °F | |
Termopol Termoton® V2GA0065A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
Nozzle Temperature | 185 - 275 °C | 365 - 527 °F | Average value: 234 °C Grade Count:22 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |
|||
Nozzle Temperature | 185 - 210 °C | 365 - 410 °F | Injection |
Huntsman IROGRAN® A 85 D 4968 Polyester-Based TPU-Injection Extrusion Grade High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman |
|||
Nozzle Temperature | 185 - 210 °C | 365 - 410 °F | Injection |
Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester Introduction: IROGRAN A 85 D 5001 DP is a antistatic, polyester based thermoplastic polyurethane intended for extrusion applications and injection molding. IROGRAN A 85 D 5001 DP is part of the HUNT.. |
|||
Nozzle Temperature | 185 - 195 °C | 365 - 383 °F | Injection Molding |
Kolon ELLAS K-385A Ether Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Cable Sheathing, High pressure tubeWheelCaster Information provided by API-Kolon. |
|||
Nozzle Temperature | 185 - 195 °C | 365 - 383 °F | Injection Molding |
Kolon ELLAS K-480A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionCompoundingIndustry PartsParts for Automobile/Mobile phoneAcetal Compound Information provided by API-Kolon. |
|||
Nozzle Temperature | 185 - 195 °C | 365 - 383 °F | Injection Molding |
Kolon ELLAS K-787A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Nozzle Temperature | 185 - 195 °C | 365 - 383 °F | |
Huntsman AVALON® 85 AB Thermoplastic Polyurethane Introduction: AVALON 85 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Nozzle Temperature | 185 - 195 °C | 365 - 383 °F | |
Huntsman AVALON® 95 AB Thermoplastic Polyurethane Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Nozzle Temperature | 185 - 200 °C | 365 - 392 °F | Injection |
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether Introduction: IROGRAN A 85 P 4441 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 85 P 4441 is part of the HUNTSMAN technical ext.. |
|||
Nozzle Temperature | 185 - 200 °C | 365 - 392 °F | |
Lubrizol Estane® S392A Thermoplastic Polyurethane Type: Estane® S392A is a Shore 93A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion, Blow .. |
|||
Nozzle Temperature | 185 - 204 °C | 365 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8058BL Thermoplastic Elastomer Elastocon® 8058BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058BL is well sui.. |
|||
Nozzle Temperature | 185 - 204 °C | 365 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8058HL Thermoplastic Elastomer Elastocon® 8058HL is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058HL is FDA compliant a.. |
|||
Nozzle Temperature | 185 - 210 °C | 365 - 410 °F | |
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Nozzle Temperature | 185 - 210 °C | 365 - 410 °F | |
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Nozzle Temperature | 185 - 210 °C | 365 - 410 °F | |
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Nozzle Temperature | 185 - 210 °C | 365 - 410 °F | |
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Nozzle Temperature | 185 - 204 °C | 365 - 400 °F | |
Elastocon TPE Technologies Elastocon® 8150B Thermoplastic Elastomer Elastocon® 8150B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8150B is well suited for consumer goods a.. |
|||
Nozzle Temperature | 185 - 210 °C | 365 - 410 °F | |
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer A hard, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Nozzle Temperature | 185 - 220 °C | 365 - 428 °F | Injection |
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Nozzle Temperature | 185 - 220 °C | 365 - 428 °F | Injection |
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Nozzle Temperature | 185 - 220 °C | 365 - 428 °F | Injection |
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Nozzle Temperature | 185 °C | 365 °F | Die |
DuPont Appeel® LSR 2044 Modified EVA Lidding Sealing Resin Appeel® 2044 is a blown or cast film resin designed to be a sealing layer for lidding applications. It provides a peelable seal over a broad temperature range to a number of container materials inc.. |