Elastocon TPE Technologies Elastocon® 2810 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Elastocon TPE Technologies
Trade Name Elastocon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastocon TPE Technologies Elastocon® 2810 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elastocon® 2810 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2810 is FDA compliant and well suited for consumer goods and industrial applications requiring non-slip/soft touch ergonomics and resilience. Elastocon® 2810 can be overmolded onto polypropylene.Information provided by Elastocon® TPE Technologies
Physical Properties Metric English Comments
Specific Gravity 0.860 g/cc
0.860 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.022 - 0.032 cm/cm
0.022 - 0.032 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 10
10
ASTM D2240
Tensile Strength, Yield 1.57 MPa
227 psi
ASTM D412
Elongation at Break 575 %
575 %
ASTM D412
100% Modulus 0.000496 GPa
0.0720 ksi
ASTM D412
Compression Set 9.0 %

@Time 79200 sec
9.0 %

@Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Feed Temperature <= 79.0 °C
<= 174 °F
Rear Barrel Temperature 138 - 160 °C
280 - 320 °F
Front Barrel Temperature 166 - 182 °C
330 - 360 °F
Nozzle Temperature 182 - 204 °C
360 - 400 °F
Mold Temperature 15.6 - 48.9 °C
60.0 - 120 °F
Back Pressure 0.345 - 0.689 MPa
50.0 - 100 psi
Descriptive Properties Value Comments
Injection Rate Fast