Material Notes:
BLUE RIVER COATINGGS WOOD PRIMER is a high quality, single component primer, not requiring any catalyzing agent. WOOD PRIMER offers good coverage, excellent durability, and ease of application, as well as being a low VOC and EPA compliant coating. BLUE RIVER COATINGS WOOD PRIMER has been tested and approved by the Window Door Manufacturer Association (WDMA). Enviromental Advantages:BLUE RIVER COATINGS WOOD PRIMER is a low VOC (Volatile Organic Compound), high performance production coating. It is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated; dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling. Characteristics: Excellent exterior durabilityExcellent hardness/impact resistanceExcellent mar and abrasion resistance Excellent adhesion to wood preservativesSolvent resistantCan be applied in a wide variety of temperature and humidity conditions without the use of retardersDistilled water is used for reductionWater is used for clean-upNon-HazardousAir dry or force curing preferredCan be oven bakedWide range of colorsShelf life of 1 yearUnused paint can be returned to containerWill not support combustionExcellent water repellencyHousehold cleaner resistantUsesWood windows and doorsPre-Finished siding Salt Fog in Harshaw No. 22 cabinet via ASTM B117 procedures with 5% NaCl solution. Evaluation of panels follows ASTM D610, D714, and D1654-Passed 500 hours.Primer has been tested and approved for use by Sealrite Windows, Inc., including an actual 18-month exterior weather test at the Sealrite plant in Nebraska. Also approved by Windsor Windows in Iowa and North Carolina.Information provided by Blue River Coatings
Physical Properties Metric English Comments
Specific Gravity >= 1.00 g/cc
>= 1.00 g/cc
Density 1.241 g/cc
0.04485 lb/in³
Solids Content 40.62 %
40.62 %
by volume
43.2 %
43.2 %
by weight
Volatile Organic Compounds (VOC) Content 240 g/l
240 g/l
pH 7.0 - 8.5
7.0 - 8.5
Mechanical Properties Metric English Comments
Impact Test 9.04 J
6.67 ft-lb
Thermal Properties Metric English Comments
Boiling Point 169 °C
336 °F
Flash Point 65.6 °C
150 °F
Processing Properties Metric English Comments
Cure Time 6.00 min

@Temperature 140 °C
0.100 hour

@Temperature 284 °F
Dry to stack, at 50% humidity
10.0 min

@Temperature 75.0 °C
0.167 hour

@Temperature 167 °F
Dust Free, at 50% humidity
19.8 min

@Temperature 75.0 °C
0.330 hour

@Temperature 167 °F
Recoat, at 50% humidity
30.0 min

@Temperature 75.0 °C
0.500 hour

@Temperature 167 °F
Dry to handle, at 50% humidity and 75°C
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesion Excellent; preservative treated wood.
Evaporation Rate Slower than ether
Theoretical Coverage 652 ft2 at 1 mil
Vapor Density Heavier than air
Water Submersion <1% water gain when submerged for 24 hours