Polymer Property : Cure Time = 42.0 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 6.00 - 42.0 min

@Temperature 25.0 °C
0.100 - 0.700 hour

@Temperature 77.0 °F
De-mold Time
Northstar Polymers MPG-D70A Room-Temperature-Curable Polyurethane Casting Elastomer
MPG-D70A is room-temperature-curable polyurethane casting elastomer system designed for molding polyurethane parts with tough, but flexible physical characteristics. The typical applications for th..