Material Notes:
3M Scotchkote Fusion-Bonded Epoxy Coating 206N (Fluid Bed Grade) is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of metal. The epoxy is applied to preheated steel as a dry powder which melts and cures to form a continuous, insulative corrosion barrier on pipe, fittings, valves, couplers, pumps and other equipment. Scotchkote coating 206N is NSF/ANSI 61 certified for potable water applications and is also resistant to corrosive soils, hydrocarbons, harsh chemicals and sea water.Information provided by 3M
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
Water Absorption <= 3.0 %
<= 3.0 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Barcol 18
18
ASTM D2583
Tensile Strength at Break 26.9 MPa
3900 psi
ASTM D2370
Elongation at Break 6.9 %
6.9 %
ASTM D2370
Compressive Strength 80.0 MPa
11600 psi
ASTM D695
Gardner Impact 18.1 J
13.3 ft-lb
1.6 cm diamter tup, 0.32cm x 7.6cm x 7.6cm steel panel
Coefficient of Friction 10.8
10.8
AP RP5L2-1968
Abrasion 0.114
0.114
[g] CS-17 1000g weight, 5000 cycles; ASTM D4060
Electrical Properties Metric English Comments
Volume Resistivity 1.30e+15 ohm-cm
1.30e+15 ohm-cm
ASTM D257
Dielectric Strength 45.3 kV/mm
1150 kV/in
ASTM D1000
Processing Properties Metric English Comments
Cure Time 3.00 min

@Temperature 246 °C
0.0500 hour

@Temperature 475 °F
4.00 min

@Temperature 232 °C
0.0667 hour

@Temperature 450 °F
6.00 min

@Temperature 218 °C
0.100 hour

@Temperature 424 °F
10.0 min

@Temperature 204 °C
0.167 hour

@Temperature 399 °F
Gel Time 0.366666 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 232 °C
0.366666 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 450 °F
0.6167 min

@Temperature 218 °C
0.6167 min

@Temperature 424 °F
0.6667 min

@Temperature 204 °C
0.6667 min

@Temperature 399 °F
2.40 min

@Temperature 246 °C
2.40 min

@Temperature 475 °F
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Blue Green