3M Scotchcast™ 5230N Electrical Epoxy Powder Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer 3M
Trade Name Scotchcast™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchcast™ 5230N Electrical Epoxy Powder Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M Scotchcast Electrical Resin 5230N is a widely used, general purpose epoxy powder resin. A one-part, blue pigmented, rapid heat-curing product, it is designed to provide a continuous, tough moisture and chemical resistant dielectric coating to a variety of substrates. Scotchcast 5230N is manufactured by a fusion blend process, insuring that each individual particle of powder contains all the components necessary to effect a complete cure and attain stated performance properties. Scotchcast 5230 is applied to a cold object via the electrostatic fluid bed process. The negatively charged resin particles are attracted to the grounded object to be coated. Coating thicknesses up to 25 mils may be obtained. Because of its superior charging capabilities Scotchast 5230N exhibits excellent slot penetration on motor stators and armatures. Uses for Scotchcast 5230N include moisture-proofing and insulating armatures, stator, buss bars and toroid cores.Information provided by 3M
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
cured; ASTM D794
Mechanical Properties Metric English Comments
Impact Test 18.1 J
13.3 ft-lb
12-15 mil coating 1/8" sandblasted steel panel Gardner 5/8: Radius Impact Tester
Abrasion 0.11
0.11
[g]; ASMT D4060
Thermal Properties Metric English Comments
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
ASTM E1530
Electrical Properties Metric English Comments
Dielectric Strength 39.4 kV/mm
1000 kV/in
12 to 15 mil coating; ASTM D149
Processing Properties Metric English Comments
Cure Time 3.00 min

@Temperature 232 °C
0.0500 hour

@Temperature 450 °F
6.00 min

@Temperature 204 °C
0.100 hour

@Temperature 399 °F
15.0 min

@Temperature 177 °C
0.250 hour

@Temperature 351 °F
Gel Time 0.150 - 0.640 min

@Temperature 193 °C
0.150 - 0.640 min

@Temperature 379 °F
hot plate
Shelf Life 24.0 Month

@Temperature <=16.0 °C
24.0 Month

@Temperature <=60.8 °F
Descriptive Properties Value Comments
Appearance Blue