Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Resin Technology Group TIGA 905 One-Part Silver Conductive Epoxy System

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer Resin Technology Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group TIGA 905 One-Part Silver Conductive Epoxy System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cure 6 minutes at 130°C or 3 minutes at 150°C.TIGA 905 is a stress-absorbing and electrically conductive, silver-filled epoxy adhesive recommended for solder replacement in microelectronic interconnect applications. This one-part, smooth paste formulation of refined pure silver and epoxy develops strong, durable, electrically and thermally conducting bonds and coatings between many different and dissimilar materials such as metals, ceramics, glass and plastic laminates. TIGA 905 is screen printable, and capable of in line surface mount component attach assembly operations.Information provided by Resin Technology Group.
Physical Properties Metric English Comments
Specific Gravity 3.60 g/cc
3.60 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
Shear Strength 10.3 MPa
1500 psi
Cured 6 minutes at 130°C, Al/Al
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.00040 ohm-cm
0.00040 ohm-cm
Cured 6 minutes at 130°C
Processing Properties Metric English Comments
Cure Time 3.00 min

@Temperature 150 °C
0.0500 hour

@Temperature 302 °F
6.00 min

@Temperature 130 °C
0.100 hour

@Temperature 266 °F
Pot Life 1440 min
1440 min
Descriptive Properties Value Comments
Color Silver
Viscosity Smooth paste
After mixing
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved