Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 4 = 356 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 4 180 - 190 °C
356 - 374 °F
Celanese Celcon® GB10 POM, 10% Glass Reinforced  (Unverified Data**)
Celcon® GB10 is a 10% glass bead filled grade for low shrinkage and warp resistance in large, flat, and thin walled parts.10% glass bead, low warpage, has been replaced by Hostaform® C 9021 GV3/10..
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Celcon® MR50B POM, Specialty  (Unverified Data**)
Celcon® MR50B is a specialty media resistant grade developed for improved bleach resistance and improved toughness.Improved media resistance, improved toughnessStandard reciprocating screw injectio..
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® C 9021 XAP² ™ POM  (Unverified Data**)
POM copolymerLow EmissionInformation provided by Celanese
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® S 9364 XAP² ™ POM, Impact Modified  (Unverified Data**)
Hostaform® acetal copolymer grade S 9364 XAP2 ™ is highly impact modified grade for demanding applications. Hostaform® S 9364 XAP2 ™ provides a significant improvement in impact strength and fl..
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® TF-10XAP® POM, Impact Modified  (Unverified Data**)
Hostaform® acetal copolymer TF-10 XAP® is low emission, improved flow, impact modified grade providing optimum performance in general purpose injection molding primarily for the interior automot..
Zone 4 180 - 200 °C
356 - 392 °F
Extrusion Molding
LG Chemical KEYFLEX BT 3140D Ester Type TPE
Description: Injection Molding, TPC-ET, Specialty, Low Melting Temperature, Low ModulusApplication: Masterbatch Carrier, Cable Compound BaseCAS: 37282-12-5Information provided by LG Chemical
Zone 4 180 - 195 °C
356 - 383 °F
Extrusion Molding
Kolon ELLAS K-395A Ether Based Thermoplastic Polyurethane
ApplicationsExtrusionInjection: Cable sheathing, Highly Pressurized HoseIndustry Parts Information provided by API-Kolon.
Zone 4 180 - 195 °C
356 - 383 °F
Extrusion Molding
Kolon ELLAS K-395F Ether Based Thermoplastic Polyurethane
ApplicationsExtrusionHighly Pressurized Hose Information provided by API-Kolon.
Zone 4 180 °C
356 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D855 Ethylene Acrylate
DuPont™ Appeel 20D855 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe..
Zone 4 180 °C
356 °F
Blown Film Coextrusion
DuPont™ Appeel® 22D843 Ethylene Acrylate
DuPont™ Appeel® 22D843 is a polypropylene modified ethylene acrylate resin designed to function as a masterbatch to achieve peelability in polypropylene based sealant layers. It provides peelable ..
Zone 4 180 °C
356 °F
Equate EFDC-7050 LLDPE Film Extrusion Resin
EFDC-7050 is a linear low-density polyethylene resin for tubular blown film extrusion. Films extruded from EFDC-7050 have good toughness and high tensile strength and puncture resistance. The produc..
Zone 4 180 - 190 °C
356 - 374 °F
Celanese Celcon® LU02 POM, UV Resistant
Celcon« acetal copolymer grade LU02 is UV stabilized material displaying a reduced gloss over standard UV acetal grades.Information provided by Celanese
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Celcon® M90-45H POM, UV Resistant
Celcon« M90-45H is an acetal copolymer which has been stabilized to give protection against property and color degradation in interior applications where UV exposure is anticipated.Information prov..
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Celcon® MR50B POM, Specialty
Celcon« MR50B is a specialty media resistant grade developed for improved bleach resistance and improved toughness.Information provided by Celanese
Zone 4 180 - 190 °C
356 - 374 °F
Celanese Hostaform® LU-02XAP® POM, UV Resistant
Hostaform« acetal copolymer grade LU-02 XAP« is UV stabilized material displaying a reduced gloss over standard UV acetal grades similar to LU-02. However, Hostaform« LU-02XAP« has lower volati..
Zone 4 180 - 190 °C
356 - 374 °F
Celanese Hostaform® LX90 POM, Unfilled
Preliminary Data SheetInformation provided by Celanese
Zone 4 180 - 190 °C
356 - 374 °F
Celanese Hostaform® LX90Z POM, UV Resistant
Hostaform« LX90Z specialty metallic appearance grades are an integrally colored nominal 9 melt flow rate based acetal copolymer material stabilized for use where ultraviolet radiation exposure is t..
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® S 9362 XAP² ™ POM, Impact Modified
Preliminary Data SheetInformation provided by Celanese
Zone 4 180 - 190 °C
356 - 374 °F
Celanese Hostaform® LX90Z XAP2 ™ POM, UV Resistant
Preliminary Data SheetDrying is required for this material to prevent poor appearance and performance of the part.Information provided by Celanese Corporation.
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® S 9363 POM, Impact Modified
Hostaform« acetal copolymer grade S 9363 is an impact modified grade for demanding applications. Hostaform« S 9363 provides good impact strength while improving modulus and weld line strength o..
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® S 9364 POM, Impact Modified
Hostaform« acetal copolymer grade S 9364 is highly impact modified grade for demanding applications. Hostaform« S 9364 provides a significant improvement in impact strength and flexibility over s..
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® XT 90 POM, Impact Modified
Preliminary Data SheetInformation provided by Celanese
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® S 9363 XAP2 ™ POM, Impact Modified
Preliminary Data SheetDrying is suggested to help achieve low emission performance and to counter if material has contacted moisture through improper storage and handling.Information provided by Cel..
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Celcon® MR90B POM, Specialty  (Unverified Data**)
Celcon® MR90B is a standard flow specialty media resistant grade developed for improved bleach resistance.Improved media resistance, standard grade.Standard reciprocating screw injection molding ma..
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® C 27021 XAP² ™ LS colored POM, UV Resistant  (Unverified Data**)
PolyacetalcopolymerLow Emission UV stabilizedInformation provided by Celanese
Zone 4 180 - 190 °C
356 - 374 °F
Celanese Hostaform® LX90Z POM, UV Resistant  (Unverified Data**)
Hostaform® LX90Z specialty metallic appearance grades are an integrally colored nominal 9 melt flow rate based acetal copolymer material stabilized for use where ultraviolet radiation exposure is t..
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® S 9363 XAP² ™ POM, Impact Modified  (Unverified Data**)
Hostaform® acetal copolymer grade S 9363 XAP2 ™ is an impact modified grade for demanding applications. Hostaform® S 9363 XAP2 ™ provides good impact strength while improving modulus and weld..
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® XT 90 POM, Impact Modified  (Unverified Data**)
Preliminary Data SheetHighly impact modified, improved weld lineInformation provided by Celanese
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® C 27021 XAP² ™ LS colored POM, UV Resistant
PolyacetalcopolymerInformation provided by Celanese
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® MT® SlideX™ 2404 POM, Medical Technology
POM copolymerInformation provided by Celanese