Material Notes:
Appeel® 20D875 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad temperature range to a number of container materials including PP, PS, PET and PVC. Appeel® 20D875 is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene resins. Appeel® 20D875 Lidding Sealant Resin complies with Food and Drug Administration Regulation 21 CFR 175.105 - - Adhesives. This Regulation describes adhesives that may be used as components of articles intended for use in packaging, transporting, or holding food, subject to the limitations and requirements therein.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792, ISO 1183
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 98.0 °C
208 °F
ASTM D3418, ISO 3146
Vicat Softening Point 60.0 °C
140 °F
ASTM D1525, ISO 306
Processing Properties Metric English Comments
Processing Temperature <= 285 °C
<= 545 °F
Feed Temperature 140 °C
284 °F
Blown Film Coextrusion
180 °C
356 °F
Extrusion Coating
Zone 2 150 °C
302 °F
Blown Film Coextrusion
230 °C
446 °F
Extrusion Coating
Zone 3 160 °C
320 °F
Blown Film Coextrusion
260 °C
500 °F
Extrusion Coating
Zone 4 180 °C
356 °F
Blown Film Coextrusion
270 °C
518 °F
Extrusion Coating
Zone 5 180 °C
356 °F
Blown Film Coextrusion
270 °C
518 °F
Extrusion Coating
Adapter Temperature 180 °C
356 °F
Blown Film Coextrusion
270 °C
518 °F
Extrusion Coating
Die Temperature 170 °C
338 °F
Blown Film Coextrusion
270 °C
518 °F
Extrusion Coating
Melt Temperature 150 - 190 °C
302 - 374 °F
Blown Film Coextrusion
235 - 270 °C
455 - 518 °F
Extrusion Coating
Dry Time 5.00 hour

@Temperature 55.0 °C
5.00 hour

@Temperature 131 °F