Polymer Property : Zone 4 = 195 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 4 180 - 195 °C
356 - 383 °F
Extrusion Molding
Kolon ELLAS K-385A Ether Based Thermoplastic Polyurethane
ApplicationsExtrusionInjection: Cable Sheathing, High pressure tubeWheelCaster Information provided by API-Kolon.
Zone 4 180 - 195 °C
356 - 383 °F
Extrusion Molding
Kolon ELLAS K-390A Ether Based Thermoplastic Polyurethane
ApplicationsExtrusion: Cable Sheathing, high pressure tubeInjectionElectric WireIndustry Parts Information provided by API-Kolon.
Zone 4 180 - 195 °C
356 - 383 °F
Extrusion Molding
Kolon ELLAS K-395A Ether Based Thermoplastic Polyurethane
ApplicationsExtrusionInjection: Cable sheathing, Highly Pressurized HoseIndustry Parts Information provided by API-Kolon.
Zone 4 180 - 195 °C
356 - 383 °F
Extrusion Molding
Kolon ELLAS K-395F Ether Based Thermoplastic Polyurethane
ApplicationsExtrusionHighly Pressurized Hose Information provided by API-Kolon.
Zone 4 185 - 195 °C
365 - 383 °F
Extrusion Molding
Kolon ELLAS K-470A Ester Based Thermoplastic Polyurethane
ApplicationsInjectionIndustry PartsParts for Automobile/Mobile phoneABS Compound
Zone 4 185 - 195 °C
365 - 383 °F
Extrusion Molding
Kolon ELLAS K-480A Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionCompoundingIndustry PartsParts for Automobile/Mobile phoneAcetal Compound Information provided by API-Kolon.
Zone 4 185 - 195 °C
365 - 383 °F
Extrusion Molding
Kolon ELLAS K-585A Caprolactone Based Thermoplastic Polyurethane
ApplicationsInjectionIndustry Parts Information provided by API-Kolon.
Zone 4 185 - 195 °C
365 - 383 °F
Extrusion Molding
Kolon ELLAS K-590A Caprolactone Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon.
Zone 4 185 - 195 °C
365 - 383 °F
Extrusion Molding
Kolon ELLAS K-596A Caprolactone Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon.
Zone 4 185 - 195 °C
365 - 383 °F
Extrusion Molding
Kolon ELLAS K-787A Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon.
Zone 4 185 - 195 °C
365 - 383 °F
Lubrizol Advanced Materials Pearlthane® D91F65D Thermoplastic Polyurethane Elastomer
PEARLTHANE® D91F65D is an aliphatic TPU supplied in colourless natural pellets. In addition to typical TPU properties like outstanding abrasion loss, PEARLTHANE® D91F65D offers excellent colou..
Zone 4 175 - 195 °C
347 - 383 °F
Lubrizol Advanced Materials PEARLCOAT® Activa D118K Thermoplastic Polyurethane Elastomer
PEARLCOAT® Activa D118K is a polycaprolactone copolyester based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss asp..
Zone 4 185 - 195 °C
365 - 383 °F
Injection
Lubrizol ESTANE® GP65AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 65AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Zone 4 185 - 195 °C
365 - 383 °F
Injection
Lubrizol ESTANE® GP75AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 75AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..