Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® ZHF 82AT0 Thermoplastic Polyurethane, Flame Retardant

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® ZHF 82AT0 Thermoplastic Polyurethane, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® ZHF 82AT0 NAT021 is an 82A aromatic polyether-based, non-halogen flame retardant, thermoplastic polyurethane (TPU) compound.Features: Soft, matte finished, good flame retardant properties.Uses: Wire and Cable extrusionAvailable in Europe, Middle East, Africa, India and AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ISO 2781
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 80 - 84

@Time 3.00 sec
80 - 84

@Time 0.000833 hour
ISO 868
Tensile Strength, Ultimate 24.5 MPa
3550 psi
ISO 527
Elongation at Break 620 %
620 %
ISO 527
50% Modulus 0.00410 GPa
0.595 ksi
100% Modulus 0.00490 GPa
0.711 ksi
300% Modulus 0.00820 GPa
1.19 ksi
Tear Strength 50.1 kN/m
286 pli
Nicked; ISO 34-1B
101.1 kN/m
576.9 pli
Unnicked; ISO 34-1B
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
vertical burn
Processing Properties Metric English Comments
Zone 1 160 °C
320 °F
Extrusion
Zone 2 170 °C
338 °F
Extrusion
Zone 3 175 °C
347 °F
Extrusion
Zone 4 180 °C
356 °F
Extrusion
Adapter Temperature 180 °C
356 °F
5, Extrusion
Die Temperature 170 °C
338 °F
7, tip, Extrusion
175 °C
347 °F
6, Extrusion
Drying Temperature 105 °C
221 °F
Dry Time 3.00 hour
3.00 hour
Dew Point -40.0 °C
-40.0 °F