DuPont Elvaloy® 2112 AC Ethylene and 12% Ethyl Acrylate Copolymer

Category Polymer , Film , Thermoplastic
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Elvaloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvaloy® 2112 AC Ethylene and 12% Ethyl Acrylate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvaloy® 2112 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for tubing is various applications. The material also is recommended for contour extrusion, as well as for blow molding of toys, gaskets and other parts requiring flexibility, stress cracking resistance and low temperature toughness. Elvaloy® 2112 AC also can be used in film applications where softness and flexibility are needed.Elvaloy® 2112 AC has a wide processing latitude in molding and extrusion equipment. EEA is very heat stable and does not give corrosive decomposition products during processing, even at the upper limit of the recommended temperature range.Information provided by DuPont.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792 - ISO 1183
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238 - ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 91
91
ASTM D2240 - ISO 868
Hardness, Shore D 35
35
ASTM D2240 - ISO 868
Tensile Strength at Break 16.0 MPa
2320 psi
500 mm/min; ASTM D638 - ISO 527-2
Elongation at Break 700 %
700 %
500 mm/min; ASTM D638 - ISO 527-2
Tensile Modulus 0.0570 GPa
8.27 ksi
1 mm/min; ASTM D638 - ISO 527-2
Thermal Properties Metric English Comments
Melting Point 99.0 °C
210 °F
By DSC; ASTM D3418 - ISO 3146
Vicat Softening Point 69.0 °C
156 °F
A<sub>50</sub> (10N); ASTM D1525 - ISO 306
Processing Properties Metric English Comments
Rear Barrel Temperature 150 °C
302 °F
Extrusion lamination and extrusion coating
150 °C
302 °F
Cast film
150 °C
302 °F
Blown film
Middle Barrel Temperature 160 °C
320 °F
Blown film
210 °C
410 °F
Cast film
220 °C
428 °F
Extrusion lamination
Front Barrel Temperature 170 °C
338 °F
Blown film
250 °C
482 °F
Cast film
290 °C
554 °F
Extrusion lamination
Adapter Temperature 180 °C
356 °F
Blown film
250 °C
482 °F
Cast Film
290 °C
554 °F
Extrusion lamination
Die Temperature 180 °C
356 °F
Blown film
250 °C
482 °F
Cast film
290 °C
554 °F
Extrusion lamination
Melt Temperature 160 - 220 °C
320 - 428 °F
For blow molding
Descriptive Properties Value Comments
EA-Content 12 wt.%
DuPont Method