Borealis Borstar® ME3441 Yellow Medium Density Polyethylene for Natural Gas Pipes

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Extruded
Manufacturer Borealis
Trade Name Borstar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borstar® ME3441 Yellow Medium Density Polyethylene for Natural Gas Pipes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borstar ME3441 is a yellow, bimodal, cadmium free, medium density polyethylene compound classified as a MRS 8.0 material (PE80) produced with the advanced Borstar technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal stability and UV-resistance and resistance to gas condensate. It also shows excellent resistance to rapid crack propagation and slow crack growth.Borstar ME3441 is recommended for pressure pipe systems in the application fields of rapid crack propagation and slow crack growth. Thanks to the structure, it gives outstanding extrudability, compared to conventional PE80 products.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
ISO 1183
Environmental Stress Crack Resistance >= 2000 hour

@Temperature 80.0 °C
>= 2000 hour

@Temperature 176 °F
At 8 bar; ISO 13479
Melt Flow 0.80 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.80 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.00 MPa
2755 psi
At 50 mm/min; ISO 527-2
Elongation at Break >= 600 %
>= 600 %
ISO 527-2
Tensile Modulus 0.800 GPa
116 ksi
At 1 mm/min; ISO 527-2
Processing Properties Metric English Comments
Front Barrel Temperature 180 - 210 °C
356 - 410 °F
Die Temperature 200 - 210 °C
392 - 410 °F
Melt Temperature 200 - 220 °C
392 - 428 °F
Head Temperature 200 - 210 °C
392 - 410 °F
Descriptive Properties Value Comments
Resistance to Rapid Crack Propagation, BAR 7
ISO 13477, Pc at 0°C, S4 / pipe size 250 mm SDR 11