Taiwan PU Corporation TPUI-G90 High Wear Resistance, Injection Molding Polycaprolactone Base TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer Taiwan PU Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation TPUI-G90 High Wear Resistance, Injection Molding Polycaprolactone Base TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic Polyurethane (TPU), High Wear Resistance, Polycaprolactone Base, Injection MoldingInformation provided by Taiwan PU Corporation.
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
Tensile Strength at Break 41.19 MPa
5974 psi
Elongation at Break 700 %
700 %
100% Modulus 0.00740 GPa
1.07 ksi
300% Modulus 0.0147 GPa
2.13 ksi
Resilience 45
45
%, Impact Resilience
Taber Abrasion, mg/1000 Cycles 18
18
Processing Properties Metric English Comments
Feed Temperature 185 °C
365 °F
Middle Barrel Temperature 190 °C
374 °F
Compress zone
Front Barrel Temperature 195 °C
383 °F
Metering zone
Adapter Temperature 200 °C
392 °F
Die Temperature 200 °C
392 °F