Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BCC Products BC 84 PVA Parting

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer BCC Products
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products BC 84 PVA Parting.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BC 84 PVA Parting/Green is a water/alcohol solution of water soluble, film forming materials. It is particularly recommended as a parting layer for separation between polyester or epoxy resins and various mold surfaces. BC 84 is normally applied by spraying on the mold surface and dries at room temperature to form a smooth, very glossy film. It will not shrink and pull away from corners or curved surfaces. After drying of the resin the film parts easily from the mold and is readily dissolved from the molded parts with water. Porous mold must first be sealed with lacquer or similar coating. A good surface on plaster may be obtained with automobile type primer-sealers and lacquers. Plaster molds must first be thoroughly dried. Metal or plastic molds should be free of other parting agents, especially silicone types. Cleaning with fine steel wool or sandpaper will not affect the high gloss obtained with BC 84. Deep scratches or pits will fill with BC 84 solution and increase the drying time.Information provided by BCC Products, Inc.
Processing Properties Metric English Comments
Pot Life 15 - 30 min

@Temperature 24.0 °C
15 - 30 min

@Temperature 75.2 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved