Material Notes:
BC 5008-2 is a very low viscosity, modified, unfilled, room temperature curing, general purpose resin system. BC 5008-2 is a clear, amber, medium pot life material, with heat resistance to 175ºF. Also considered an excellent general purpose adhesive for in-shop use and will function as a laminating system for horizontal surfaces.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Brookfield Viscosity 550 cP

@Temperature 23.9 °C
550 cP

@Temperature 75.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 86

@Temperature 23.9 °C
86

@Temperature 75.0 °F
Tensile Strength, Ultimate 65.5 MPa
9500 psi
Flexural Strength 124 MPa
18000 psi
Compressive Strength 120 MPa
17400 psi
Thermal Properties Metric English Comments
CTE, linear 21.2 µm/m-°C
11.8 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 70.6 °C
159 °F
Processing Properties Metric English Comments
Cure Time 480 - 720 min

@Temperature 24.0 °C
8.00 - 12.0 hour

@Temperature 75.2 °F
Pot Life 25 - 30 min

@Temperature 24.0 °C
25 - 30 min

@Temperature 75.2 °F
1/2 lb mass
Descriptive Properties Value Comments
Mix Ratio 100:25 by weight, 100:26 by volume