Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total HDPE B5845 High Density Polyethylene - Blow Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Total Atofina
Trade Name HDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total HDPE B5845 High Density Polyethylene - Blow Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bimodal HDPE Blow Molding ResinCharacteristics:Excellent stress cracking resistanceExcellent stiffnessApplications:Household chemicalsIndustrial chemicalsIndustrial partsFood packagingPersonal care packagesInformation provided by Total Petrochemicals.
Physical Properties Metric English Comments
Density 0.958 g/cc
0.0346 lb/in³
ASTM D792
ESCR 100% Igepal® >= 800 hour
>= 800 hour
ASTM D1693, Cond. B
ESCR 10% Igepal® >= 300 hour
>= 300 hour
ASTM D1693, Cond. B
Melt Flow 0.45 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.45 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.3 MPa
4400 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Processing Properties Metric English Comments
Processing Temperature 182 - 204 °C
360 - 400 °F
Blow Molding Stock Temp.
Melt Temperature 193 - 216 °C
380 - 420 °F
Extrusion
Descriptive Properties Value Comments
Process Blow Molding
Region US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: