Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ASTM E 831 |
DuPont Performance Polymers Delrin® 100AF Acetal Homopolymer
(Unverified Data**) Delrin® 100AF is a high viscosity acetal homopolymer containing 20% Teflon® PTFE fibers. It is designed for applications requiring low wear and/or low friction against steel, itself, and other pla.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 127UV BK701 Acetal Homopolymer
(Unverified Data**) Delrin® 127UV BK701 is a high viscosity, UV stabilized acetal homopolymer. It has excellent impact strength, UV resistance and thermal stability. It is well suited for automotive interior applicati.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 527UVE RD402 Acetal Homopolymer
(Unverified Data**) Delrin® 527UVE RD402 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers, pigmented red, having extremely low VOC emissions, developed for automotive interior applicatio.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500P is a medium viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information p.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 55.0 - 160 °C |
61.1 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) Minlon® 10B40HS1 BK061 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 55.0 - 160 °C |
61.1 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 100 - 200 °C |
61.1 µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 80.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 40.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 40.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Asia Pacific) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 40.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Asia Pacific) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 40.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Europe-Africa-Middle East) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 40.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Asia Pacific) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -30.0 - 30.0 °C |
61.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**) Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 23.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**) Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -30.0 - 30.0 °C |
61.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**) Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 23.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**) Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -30.0 - 30.0 °C |
61.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -30.0 - 30.0 °C |
61.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -30.0 - 30.0 °C |
61.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66
(Unverified Data**) Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 23.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66
(Unverified Data**) Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 100PE NC010A Acetal Homopolymer Delrin® 100PE NC010A is a high viscosity acetal homopolymer, an enhanced version of Delrin® 100P with extremely low VOC emissions. It has improved processing thermal stability, good mechanical pro.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 100 - 200 °C |
61.1 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Chevron Phillips Xtel® XK2240 Polyphenylene Sulfide Alloy
(discontinued **) Natural Color Polyphenylene Sulfide AlloyXtel™ XK2240 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of tough.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 527UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 527UVE NC010 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information p.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG100P is a high viscosity acetal homopolymer, with improved thermal stability for use in easy to fill molds. It has been developed for consideration into applications such as parts for the.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 149 - 249 °C |
61.1 µin/in-°F @Temperature 300 - 480 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 100 - 200 °C |
61.1 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel PPA resins, ET-1000 HS offers high fatigue str.. |