Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 100 - 200 °C |
61.1 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 100 - 200 °C |
61.1 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AE-8133 Polyphthalamide (PPA)
(discontinued **) Amodel AE-8133 is a 33% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temperature, high flexural.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 100AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100AL NC010 an unreinforced, high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication for low wear and friction against metals and plastics.Informat.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 100TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100TL NC010 is a high viscosity acetal homopolymer with 1.5% Teflon® PTFE Micropowder.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 127UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 127UVE NC010 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information pro.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 300CP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of processing and part performance.Information provided by DuPont Perf.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500P is a medium viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information p.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 55.0 - 160 °C |
61.1 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) Minlon® 10B40HS1 BK061 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 55.0 - 160 °C |
61.1 µin/in-°F @Temperature 131 - 320 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) Minlon® 10B40HS1 BK061 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 100 - 250 °C |
61.1 µin/in-°F @Temperature 212 - 482 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 80.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East) VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 40.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC 30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 40.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 40.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Asia Pacific) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 40.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Asia Pacific) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 40.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Europe-Africa-Middle East) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 40.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Europe-Africa-Middle East) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 100 - 200 °C |
61.1 µin/in-°F @Temperature 212 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 150 °C |
61.1 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 40.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 40.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Asia Pacific) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 40.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 100 - 200 °C |
61.1 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
Chevron Phillips Xtel® XK2340 Polyphenylene Sulfide Alloy Black Polyphenylene Sulfide AlloyXtel™ XK2340 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of toughness and.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 23.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**) Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -40.0 - 23.0 °C |
61.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**) Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature -30.0 - 30.0 °C |
61.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
DAM; ASTM E 831 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 100PE NC010A Acetal Homopolymer Delrin® 100PE NC010A is a high viscosity acetal homopolymer, an enhanced version of Delrin® 100P with extremely low VOC emissions. It has improved processing thermal stability, good mechanical pro.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 527UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 527UVE NC010 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information p.. |
|||
CTE, linear, Transverse to Flow | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG100AL is a high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication. It has been developed for consideration into applications such as parts for t.. |