Polymer Property : Thermal Conductivity = 0.200 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.200 W/m-K

@Temperature 400 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 752 °F
Pyrotek Insural® 85 MASTIC Insulating Mastic for Aluminum contact Applications
Insural® 85 MASTIC is an asbestos-free, durable and insulating refractory composition designed for the fabrication of launders and jointing, bedding and patching of precast refractory shapes.Advant..
Thermal Conductivity 0.200 W/m-K

@Temperature 400 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 752 °F
Pyrotek Insural® GP MASTIC Insulating mastic for general-purpose refractory applications
Insural® GP Mastic is an asbestos-free, durable and insulating refractory fiber composition designed for general-purpose patching and veneering applications that are not exposed to contact with mol..
Thermal Conductivity 0.200 W/m-K

@Temperature 300 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 572 °F
(DIN 51046)+
Pyrotek Pyrite B-3 Refractory Board
Pyrotek B-3 is a highly versatile calcium silicate board for use in a variety of machined shapes and general purpose applications. Among its uses, Pyrotek B-3 is established as the industry standar..
Thermal Conductivity 0.200 W/m-K

@Temperature 500 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 932 °F
(DIN 51046)+
Pyrotek Pyrite B-3 Refractory Board
Pyrotek B-3 is a highly versatile calcium silicate board for use in a variety of machined shapes and general purpose applications. Among its uses, Pyrotek B-3 is established as the industry standar..
Thermal Conductivity 0.200 W/m-K

@Temperature 540 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Pyrotek SF-50 Foamed Fused Silica Insulation Board
SF-50 is characterized by its uniform open cell structure which allows it to be machined to close tolerances. It can be drilled, sawed or modified with conventional tools. For quick construction o..
Thermal Conductivity 0.200 W/m-K

@Temperature 760 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1400 °F
Pyrotek Pyrocast L-40 Insulating Refractory
Pyrocast L-40 is a fiber free refractory moldable designed for use in contact with molten aluminum. L-40 has excellent workability for use as an insulating lining or patching material.Recommended C..
Thermal Conductivity 0.200 W/m-K

@Temperature 100 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
3M Dyneon™ CCX6380 PTFE, 10% Polyimide Filler  (discontinued **)
Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div..
Thermal Conductivity 0.200 - 0.300 W/m-K

@Temperature 100 °C
1.39 - 2.08 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 125 R GM Refractory Insulating Castable
Description: Golite 125 R GM has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products.Informati..
Thermal Conductivity 0.200 W/m-K

@Temperature 816 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Mid-Mountain Materials CERMEX® MT1800 Needled Silica Mat
CERMEX® MT1800 Needled Silica Blanket is a binderless material comprised of high purity, amorphous silica fibers. In demanding applications, the abrasion and vibration resistance of this mat make..
Thermal Conductivity 0.200 W/m-K

@Temperature 600 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1110 °F
BS 1902 Section 5.5 1991
Skamol Group Moler 10 Aggregate Insulation
SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre..
Thermal Conductivity 0.200 W/m-K

@Temperature 600 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1110 °F
BS 1902 Section 5.5 1991
Skamol Group Moler 5 Aggregate Insulation
SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre..
Thermal Conductivity 0.200 W/m-K

@Temperature 600 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1110 °F
BS 1902 Section 5.5 1991
Skamol Group Moler BB-Filler Aggregate Insulation
SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre..
Thermal Conductivity 0.200 W/m-K

@Temperature 600 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C-182
Skamol Group Moler ROTOL Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Thermal Conductivity 0.200 W/m-K

@Temperature 200 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 392 °F
Mean temp.; ASTM C-201 supplemented by ASTM C-182
Skamol Group SKAMOCAST 112-80 Insulating Castable
SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f..
Thermal Conductivity 0.200 W/m-K

@Temperature 982 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1800 °F
Thermal Ceramics Ceraboard 100
Ceraboard is a refractory fibre board supplied in panels of standard thicknesses made from a slurry of refractory fibres and binders which have a low organic content.Features: High temperature stabi..
Thermal Conductivity 0.200 W/m-K

@Temperature 982 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1800 °F
Thermal Ceramics Ceraboard P
Ceraboard P has tighter thickness tolerances and s particularly useful in applications requiring very low variability. It is made from a slurry of refractory fibers and binders which have a low orga..
Thermal Conductivity 0.200 W/m-K

@Temperature 1090 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 2000 °F
Thermal Ceramics Kaowool Flex-Wrap Paper
Kaowool Flex-Wrap is produced from a blend of Kaowool high purity ceramic fibers and organic binders in a unique paper making process. Due to its low organic binder content, offgassing is at a minim..
Thermal Conductivity 0.200 W/m-K

@Temperature 400 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 752 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics SALI Alumina Insulation
SALI has been serving 1700°C low mass furnace users longer than any other alumina fiber board available today. SALI is a premium grade rigid fiber board with superior hot strength.Information provi..
Thermal Conductivity 0.200 W/m-K

@Temperature 1010 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1850 °F
Zircar Refractory Composites RSBD-LD ALUMINA-SILICA INSULATION
ZRCI Alumina-Silica Insulation Type RSBD-LD Board is a ceramic fiber insulation suitable for use to 1260°C (2300°C). It is a strong, rigid refractory structure of high temperature ceramic fibers a..
Thermal Conductivity 0.200 W/m-K

@Temperature 800 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1470 °F
ASTM C177
Zircar Refractory Composites RS-C ALUMINA-SILICA MOLDABLE
ZIRCAR Alumina-Silica Insulating Blanket Type RS-C Moldable is composed of long, high strength ceramic fibers, with an inorganic alumina binder/rigidizing agent. It is a wet blanket that is shipped ..
Thermal Conductivity 0.200 W/m-K

@Temperature 800 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation
Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo..
Thermal Conductivity 0.200 W/m-K

@Temperature 816 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Tritex TRI-F Blanket Insulation
TRI-F is a unique thermal and acoustic insulation that combines three high temperature fibers in a patented process. The result is a blanket with a service life to 1500°F. By blending fibers of var..
Thermal Conductivity 0.200 W/m-K

@Temperature 816 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C182
BNZ Materials BNZ-23A Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.200 W/m-K

@Temperature 816 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C182
BNZ Materials BNZ-24 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.200 W/m-K

@Temperature 400 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 752 °F
ASTM C182
BNZ Materials BNZP-23B Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.200 W/m-K

@Temperature 400 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 752 °F
ASTM C182
BNZ Materials BNZP-26A Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.200 W/m-K

@Temperature 260 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 500 °F
ASTM C182
BNZ Materials PA 20 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.200 W/m-K

@Temperature 816 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Thermal Ceramics Kaomat SL Blanket
Thermal Ceramics Kaomat insulation is a non-woven needle-felted "E" fiberglass mat. Kaomat is an economical insulating material used extensively in both the marine and commercial insulation markets...
Thermal Conductivity 0.200 W/m-K

@Temperature 1100 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 2010 °F
ASTM C177-76
Zircar Ceramics ASH Alumina-Silica Insulation
ZIRCAR Ceramics Alumina-Silica Insulation Type ASH is one of the first alumina-silica products produced by ZIRCAR. Made of bulk fiber and inorganic alumina binders Type ASH is uniform throughout its..
Thermal Conductivity 0.200 W/m-K

@Temperature 800 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation
Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo..