Mid-Mountain Materials CERMEX® MT1800 Needled Silica Mat

Category Ceramic , Glass , Glass Fiber , Oxide , Silicon Oxide , Other Engineering Material , Composite Fibers
Manufacturer Mid-Mountain Materials
Trade Name CERMEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mid-Mountain Materials CERMEX® MT1800 Needled Silica Mat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CERMEX® MT1800 Needled Silica Blanket is a binderless material comprised of high purity, amorphous silica fibers. In demanding applications, the abrasion and vibration resistance of this mat makes this material superior to other products manufactured from shot-containing fibers. The complete absence of shot and organic binders make this product superior in performance in severe environments where vibration can often degrade shot containing materials. The amorphous silica fibers that make up CERMEX® MT1800 mat are unaffected by most chemicals, except strong alkalis, hydrofluoric acid or sodium. Inherent to the chemistry, the silica fibers will have a tendency to shrink on initial exposure to elevated temperatures. For most industrial applications, this does not pose a problem. However, in applications where dimensional stability is critical (at elevated temperatures), CERMEX® MT1800 is available in a pre-shrunk (fired) version.Information provided by Mid-Mountain Materials
Physical Properties Metric English Comments
Density 0.136 - 0.152 g/cc
0.00492 - 0.00550 lb/in³
Filament Diameter 6.0 - 9.0 µm
6.0 - 9.0 µm
Thickness 6350 microns
250 mil
12700 microns
500 mil
25400 microns
1000 mil
Thermal Properties Metric English Comments
Thermal Conductivity 0.0648 W/m-K

@Temperature 260 °C
0.450 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.112 W/m-K

@Temperature 538 °C
0.777 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.200 W/m-K

@Temperature 816 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1500 °F
0.278 W/m-K

@Temperature 982 °C
1.93 BTU-in/hr-ft²-°F

@Temperature 1800 °F
Melting Point 1704 °C
3099 °F
Maximum Service Temperature, Air 982 °C
1800 °F
Continuous
1260 °C
2300 °F
Intermittent
Component Elements Properties Metric English Comments
SiO2 >= 96 %
>= 96 %
Descriptive Properties Value Comments
Roll Length (ft) 116
1/4" (350 ft<sup>2</sup>/roll)
33
1" (100 ft<sup>2</sup>/roll)
58
1/2" (175 ft<sup>2</sup>/roll)
Shot Content (%) None
Width (in) 36