Material Notes:
SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on fired Moler aggregates, refractory materials, or exfoliated vermiculiteEffective insulationQuick and economical installationUsed as monolithic heat insulation in a wide range of industrial kilns and furnaces, boilers, chimneys, and fluesThe Vermicast grades are favored as infill in aluminum reduction cell cathodes due to their non-wetting capacity to molten metal and good bath resistance.Information provided by Skamol.
Physical Properties Metric English Comments
Bulk Density 0.545 g/cc
0.0197 lb/in³
As Supplied
0.801 g/cc
0.0289 lb/in³
Defined by casting method, +/- 50kg (110 lbs)
Loss On Ignition 6.00 %

@Temperature 1025 °C
6.00 %

@Temperature 1877 °F
Porosity 68 %
68 %
Mechanical Properties Metric English Comments
Compressive Strength 2.90 MPa
421 psi
Dried at 110°C (230°F)
Thermal Properties Metric English Comments
Thermal Conductivity 0.200 W/m-K

@Temperature 200 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 392 °F
Mean temp.; ASTM C-201 supplemented by ASTM C-182
0.220 W/m-K

@Temperature 400 °C
1.53 BTU-in/hr-ft²-°F

@Temperature 752 °F
ASTM C-201 supplemented by ASTM C-182
0.240 W/m-K

@Temperature 600 °C
1.67 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C-201 supplemented by ASTM C-182
Maximum Service Temperature, Air 900 °C
1650 °F
Shrinkage 1.50 %

@Time 43200 sec
1.50 %

@Time 12.0 hour
Linear Reheat Shrinkage, 12h at 100°C (180°F) below max. service temp.
Component Elements Properties Metric English Comments
Al2O3 + TiO2 14.5 %
14.5 %
CaO 7.0 %
7.0 %
Fe2O3 8.0 %
8.0 %
K2O+Na2O 1.0 %
1.0 %
MgO 1.0 %
1.0 %
SiO2 62 %
62 %
Descriptive Properties Value Comments
Pyrometric Cone Equivalent 1200°C
ASTM C24-89, ORTON cones