Material Notes:
TRI-F is a unique thermal and acoustic insulation that combines three high temperature fibers in a patented process. The result is a blanket with a service life to 1500°F. By blending fibers of varying diameters it gives TRI-F excellent acoustic properties, added rigidity and strength. This patented process also removes shot thereby making it ideal for applications that see excessive vibration. TRI-F is Biosafe, environmentally friendly and manufactured from 100% recycled raw materials. TRI-F is also classified by IARC as Group 3 and is not classifiable as carcinogenic to humans.Information provided by TRITEX
Physical Properties Metric English Comments
Density 2.75 - 2.90 g/cc
0.0994 - 0.105 lb/in³
Loss On Ignition <= 0.50 %
<= 0.50 %
Filament Diameter 6.0 µm
6.0 µm
Average
Absorption Coefficient 0.040

@Frequency 125 Hz
0.040

@Frequency 125 Hz
Sound
0.12

@Frequency 250 Hz
0.12

@Frequency 250 Hz
Sound
0.31

@Frequency 500 Hz
0.31

@Frequency 500 Hz
Sound
0.64

@Frequency 1000 Hz
0.64

@Frequency 1000 Hz
Sound
0.78

@Frequency 2000 Hz
0.78

@Frequency 2000 Hz
Sound
0.87

@Frequency 4000 Hz
0.87

@Frequency 4000 Hz
Sound
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 552 MPa
80000 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.0807 W/m-K

@Temperature 371 °C
0.560 BTU-in/hr-ft²-°F

@Temperature 700 °F
0.0994 W/m-K

@Temperature 482 °C
0.690 BTU-in/hr-ft²-°F

@Temperature 900 °F
0.160 W/m-K

@Temperature 649 °C
1.11 BTU-in/hr-ft²-°F

@Temperature 1200 °F
0.200 W/m-K

@Temperature 816 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Melting Point >= 1100 °C
>= 2010 °F
Fiber
Maximum Service Temperature, Air 815 °C
1500 °F
Component Elements Properties Metric English Comments
Al2O3 14 %
14 %
Primary Fiber
CaO 15 %
15 %
Primary Fiber
FeO 0.10 %
0.10 %
Primary Fiber
MgO 7.5 %
7.5 %
Primary Fiber
MnO 10 %
10 %
Primary Fiber
Other 3.4 %
3.4 %
Primary Fiber
SiO2 42 %
42 %
Primary Fiber
Descriptive Properties Value Comments
Average Fiber Length (mm) 4
Color white/beige
Moisture Resistant Yes
Surface Treatment None