Material Notes:
Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon division of 3M.
Physical Properties Metric English Comments
Specific Gravity 2.00 g/cc
2.00 g/cc
ASTM D4894
Bulk Density 0.580 g/cc
0.0210 lb/in³
ASTM D4894
Particle Size 750 µm
750 µm
ASTM D4894
Deformation 3.0 %

@Pressure 15.00 MPa
3.0 %

@Pressure 2175 psi
permanent; ASTM D621
5.0 %

@Time 86400 sec,
Pressure 15.00 MPa
5.0 %

@Time 24.0 hour,
Pressure 2175 psi
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
Initial; ASTM D2240
53

@Time 15.0 sec
53

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 18.6 MPa
2700 psi
ASTM D4894
Elongation at Break 270 %
270 %
ASTM D4894
Tensile Modulus 0.0965 GPa
14.0 ksi
ASTM D638
Thermal Properties Metric English Comments
CTE, linear 108 µm/m-°C

@Temperature 30.0 - 100 °C
60.0 µin/in-°F

@Temperature 86.0 - 212 °F
ASTM E831
139 µm/m-°C

@Temperature 100 - 200 °C
77.0 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
173 µm/m-°C

@Temperature 200 - 300 °C
96.0 µin/in-°F

@Temperature 392 - 572 °F
ASTM E831
Thermal Conductivity 0.200 W/m-K

@Temperature 100 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
0.220 W/m-K

@Temperature 250 °C
1.53 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM E1530
Shrinkage 2.4 %
2.4 %
ASTM D4894