Material Notes:
Product description: Grilon TSGK-30 X is a heat stabilized PA66 + PA6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30 X has the following important properties: Good flow behaviorHigh weld line strengthLow warpage Grilon TSGK-30 X is used typically for housing elements, relais bearers, axle spindle casings, and applications which demand medium level of stiffness and low warpage.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Water Absorption 7.0 %
7.0 %
ISO 62
Moisture Absorption 2.50 %
2.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 100 MPa
14500 psi
conditioned; ISO 2039-1
200 MPa
29000 psi
dry; ISO 2039-1
Tensile Strength at Break 85.0 MPa
12300 psi
conditioned; ISO 527-1/-2
155 MPa
22500 psi
dry; ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
dry; ISO 527-1/-2
10 %
10 %
conditioned; ISO 527-1/-2
Tensile Modulus 5.70 GPa
827 ksi
conditioned; ISO 527-1/-2
8.50 GPa
1230 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
dry; ISO 179/1eU
7.50 J/cm²
35.7 ft-lb/in²
conditioned; ISO 179/1eU
4.50 J/cm²

@Temperature 30.0 °C
21.4 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
4.50 J/cm²

@Temperature 30.0 °C
21.4 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
dry; ISO 179/1eA
1.30 J/cm²
6.19 ft-lb/in²
conditioned; ISO 179/1eA
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C
194 - 248 °F
long term; EMS
180 °C
356 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 80.0 °C
176 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 23.0 kV/mm
584 kV/in
conditioned; IEC 60243-1
24.0 kV/mm
610 kV/in
dry; IEC 60243-1
Comparative Tracking Index 425 V
425 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Interior
Electricals & Electronics Electrical appliances
Form Granules
Industry & Consumer goods Housewares
Mechanical Engineering
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Users viewing this material also viewed the following: