Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide Compound  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide Compound  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Natural Color Polyphenylene Sulfide CompoundRyton® BR42B is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surface friction and wear applications. Has a wear rate of 0.001 mm/hr as per ASTM D3702.Applications: Pump VanesComments: Test specimen molding conditions: Stock Temperature, 315-345°C; Mold Temperature, 135°C; ASTM Values Converted to SI UnitsData provided by Chevron Phillips Chemical Company LP.Solvay Specialty Polymers has acquired the Ryton product line.
Physical Properties Metric English Comments
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
102 mm X 102 mm X 3.2 mm Plaques, Edge Gated
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
Measured on 102 mm X 102 mm X 3.2 mm Plaques, Edge Gated
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 170 MPa
24700 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Flexural Yield Strength 275 MPa
39900 psi
ASTM D790
Flexural Modulus 15.0 GPa
2180 ksi
ASTM D790
Compressive Yield Strength 205 MPa
29700 psi
ASTM D695
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.90 J/cm
12.9 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.32
0.32
Against 52100 steel; 100 hours; 22.7 kg load (1.7 MPa); 36 RPM; Dry; Ambient Temperature; PV=2500; ASTM D3702
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 100 - 200 °C
6.11 µin/in-°F

@Temperature 212 - 392 °F
Axial; ASTM E831
16.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
8.89 µin/in-°F

@Temperature -58.0 - 122 °F
Axial; ASTM E831
CTE, linear, Transverse to Flow 43.0 µm/m-°C

@Temperature 20.0 °C
23.9 µin/in-°F

@Temperature 68.0 °F
ASTM E831
98.0 µm/m-°C

@Temperature 100 - 200 °C
54.4 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
Thermal Conductivity 0.330 W/m-K
2.29 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 180 °C
356 °F
UL Temperature Index per UL746B
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Annealed 2 hr @ 200°C; ASTM D654
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
Dielectric Constant 4.0

@Frequency 1000 Hz
4.0

@Frequency 1000 Hz
ASTM D150
4.0

@Frequency 1e+6 Hz
4.0

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149
Dissipation Factor 0.0030

@Frequency 1000 Hz
0.0030

@Frequency 1000 Hz
ASTM D150
0.0030

@Frequency 1e+6 Hz
0.0030

@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 150 V
150 V
UL 746A