Material Notes:
Flexible with low hardness
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Before Curing
Viscosity 20000 cP
20000 cP
Before Curing
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
After Curing
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
After Curing
Tensile Strength at Break 1.50 MPa
218 psi
After Curing
Elongation at Break 150 %
150 %
After Curing
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Processing Properties Metric English Comments
Cure Time <= 1440 min
<= 24.0 hour
Curing
Pot Life 30 min
30 min
Curing
Descriptive Properties Value Comments
Color White