CENTROPLAST CENTRO HPM Polysulfone

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTRO
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTRO HPM Polysulfone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This plastic has good hydrolysis, chemical and radiation resistance, and can operate at high temperatures. It is used in food processing industry, pumps and valves, and medical equipment.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.40 %
0.40 %
in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 0.85 %
0.85 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Hardness, Rockwell M 91

@Thickness 10.0 mm
91

@Thickness 0.394 in
ISO 2039-2
Ball Indentation Hardness 155 MPa
22500 psi
value at 30 sec.; ISO 2039-1
Tensile Strength, Yield 80.0 MPa
11600 psi
v = 50 mm/min; ISO 527-2
Elongation at Break 10 %
10 %
ISO 527-2
Tensile Modulus 2.70 GPa
392 ksi
ISO 527-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C

@Temperature 20.0 °C
33.3 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Thermal Conductivity 0.260 W/m-K
1.80 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 150 °C
302 °F
Long Term
180 °C
356 °F
Short term
Deflection Temperature at 1.8 MPa (264 psi) 170 °C
338 °F
ISO 75-2
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
HB

@Thickness 6.00 mm
HB

@Thickness 0.236 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 3.0

@Frequency 100 Hz
3.0

@Frequency 100 Hz
IEC 60250
3.0

@Frequency 1e+6 Hz
3.0

@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 30.0 kV/mm
762 kV/in
in transformer oil; IEC 60243-1
Dissipation Factor 0.0010

@Frequency 100 Hz
0.0010

@Frequency 100 Hz
IEC 60250
0.0030

@Frequency 1e+6 Hz
0.0030

@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 150 V
150 V
IEC 60112