Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | RT |
Outokumpu 4021 Martensitic Stainless Steel Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat.. |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | RT |
Outokumpu 4028 Martensitic Stainless Steel Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat.. |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | |
Misumi Alumina 99 Aluminum Oxide, Al2O3 Information provided by MISUMI Corporation. |
|||
Thermal Conductivity | 30.0 W/m-K @Temperature 85.0 °C |
208 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy 281-338 Bismuth-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | |
Sapco 99.7% Aluminum Oxide Information provided by Sapco. |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | |
Sapco 99.9% Aluminum Oxide Information provided by Sapco. |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | DIN EN 821-2 |
CeramTec RK 87 Alumina, 99.8% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | DIN EN 821-2 / ASTM-C408 |
CeramTec Rubalit® A 1999.5 Alumina, 99.7% Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon mat.. |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | DIN EN 821-2 |
CeramTec V 679 Alumina, 99.7% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Thermal Conductivity | 30.0 - 35.0 W/m-K | 208 - 243 BTU-in/hr-ft²-°F | |
Goodfellow Nickel Base Magnetic Shielding Alloy - Mu Metal High Nickel magnetically soft alloy used for magnetic shielding, high quality but low noise audio frequency transformers, ground fault interrupter cores, anti-shoplifting devices, tape recorder head.. |
|||
Thermal Conductivity | 30.0 - 32.0 W/m-K | 208 - 222 BTU-in/hr-ft²-°F | |
Goodfellow T2-Thermocouple Alloy The negative element of the type K thermocouple, the positive being T1. The thermocouple can be used up to 1250C in oxidizing atmospheres, and probably is the most common in use.Information provided.. |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | ASTM C408 |
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | ASTM-C408 |
CoorsTek AD-996 99.6% Alumina |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | ASTM C408 |
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | ASTM-C408 |
CoorsTek CAP 3 99.5% Alumina Ceramic Armor Material CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys.. |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | ASTM C408 |
CoorsTek PlasmaPure™ Alumina (nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | |
CLAL-MSX NICLAL 1800 0 Annealed Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good corrosion resistanceHigh mechanical propertiesTypical Applications:Parts subject to high stressHigh quality fastenersInformation provided by CLAL-MSX |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | |
CLAL-MSX NICLAL 1800 H12 1/2 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good corrosion resistanceHigh mechanical propertiesTypical Applications:Parts subject to high stressHigh quality fastenersInformation provided by CLAL-MSX |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | |
CLAL-MSX NICLAL 1800 H14 4/4 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good corrosion resistanceHigh mechanical propertiesTypical Applications:Parts subject to high stressHigh quality fastenersInformation provided by CLAL-MSX |
|||
Thermal Conductivity | 30.0 W/m-K @Temperature 599 °C |
208 BTU-in/hr-ft²-°F @Temperature 1110 °F |
hardened to 45 HRC |
Bohler-Uddeholm ORVAR® 2M / AISI H13 Hot Work Tool Steel Orvar 2 Microdized is a chromium-molybdenum-vanadium alloyed steelORVAR® 2M / AISI H13 is a conventionally produced hot work tool steel with overall good ductility, toughness, wear resistance, hard.. |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | |
Ceradyne Ceralloy® 13740 AlN-SiC Applications: replacement for Ceralloy® 2710 BeO-SiCterminationssever wedgesload pelletsabsorbersInformation provided by Ceradyne Company |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | |
Ceradyne Ceralloy® 6703 MgO-SiC Applications: absorbersbuttonsInformation provided by Ceradyne Company |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | DIN EN 821-2 |
CeramTec AT 79 Alumina, 99.6% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | |
Ceradyne Ceralloy® 6705 MgO-SiC Applications: absorbersbuttonsInformation provided by Ceradyne Company |