Ceradyne Ceralloy® 13740 AlN-SiC

Category Ceramic , Carbide , Nitride
Manufacturer Ceradyne Advanced Ceramics
Trade Name Ceralloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ceradyne Ceralloy® 13740 AlN-SiC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: replacement for Ceralloy® 2710 BeO-SiCterminationssever wedgesload pelletsabsorbersInformation provided by Ceradyne Company
Physical Properties Metric English Comments
Density 3.19 g/cc
0.115 lb/in³
Mechanical Properties Metric English Comments
Flexural Strength 300 MPa
43500 psi
Thermal Properties Metric English Comments
CTE, linear 5.10 µm/m-°C

@Temperature 20.0 - 1000 °C
2.83 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 30.0 W/m-K
208 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Constant 15

@Frequency 8.00e+9 Hz
15

@Frequency 8.00e+9 Hz
15

@Frequency 1e+10 Hz
15

@Frequency 1e+10 Hz
22

@Frequency 1e+9 Hz
22

@Frequency 1e+9 Hz
Dissipation Factor 0.11

@Frequency 1e+9 Hz
0.11

@Frequency 1e+9 Hz
0.28

@Frequency 1e+10 Hz
0.28

@Frequency 1e+10 Hz
0.30

@Frequency 8.00e+9 Hz
0.30

@Frequency 8.00e+9 Hz
Descriptive Properties Value Comments
Composition AlN+40%SiC