Material Notes:
The negative element of the type K thermocouple, the positive being T1. The thermocouple can be used up to 1250C in oxidizing atmospheres, and probably is the most common in use.Information provided by Goodfellow.Composition Notes: Al + Mn + Si content 5 wt%.
Physical Properties Metric English Comments
Density 8.50 - 8.70 g/cc
0.307 - 0.314 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 550 - 780 MPa
79800 - 113000 psi
Elongation at Break <= 44 %
<= 44 %
Izod Impact, Unnotched 1.08 J/cm
2.02 ft-lb/in
Notch Status Unknown
Thermal Properties Metric English Comments
CTE, linear 16.8 µm/m-°C

@Temperature 20.0 - 1000 °C
9.33 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 30.0 - 32.0 W/m-K
208 - 222 BTU-in/hr-ft²-°F
Melting Point 1315 - 1390 °C
2399 - 2530 °F
Solidus 1315 °C
2399 °F
Liquidus 1390 °C
2530 °F
Maximum Service Temperature, Air 1100 °C
2010 °F
Component Elements Properties Metric English Comments
Nickel, Ni 95 %
95 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000290 - 0.0000330 ohm-cm
0.0000290 - 0.0000330 ohm-cm
Temperature Coefficient of 0.0019/K