| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 3.90 g/cc | 0.141 lb/in³ | |
| Water Absorption | 0.000 % | 0.000 % |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 340 MPa | 49300 psi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 7.50 µm/m-°C @Temperature 20.0 - 600 °C |
4.17 µin/in-°F @Temperature 68.0 - 1110 °F |
|
| 9.90 µm/m-°C @Temperature 20.0 - 800 °C |
5.50 µin/in-°F @Temperature 68.0 - 1470 °F |
||
| Thermal Conductivity | 30.0 W/m-K | 208 BTU-in/hr-ft²-°F | |
| Melting Point | 2200 °C | 3990 °F | |
| Maximum Service Temperature, Air | 1500 °C | 2730 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 99.7 % | 99.7 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | |
| Dielectric Constant | 10.0 | 10.0 | |
| Dielectric Strength | >= 10.0 kV/mm | >= 254 kV/in |