Material Notes:
Applications: absorbersbuttonsInformation provided by Ceradyne Company
Physical Properties Metric English Comments
Density 3.50 g/cc
0.126 lb/in³
Mechanical Properties Metric English Comments
Flexural Strength 200 MPa
29000 psi
Thermal Properties Metric English Comments
CTE, linear 15.4 µm/m-°C

@Temperature 20.0 - 1000 °C
8.56 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 30.0 W/m-K
208 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Constant 10.9

@Frequency 1.20e+10 Hz
10.9

@Frequency 1.20e+10 Hz
11.1

@Frequency 1e+10 Hz
11.1

@Frequency 1e+10 Hz
11.2

@Frequency 8.00e+9 Hz
11.2

@Frequency 8.00e+9 Hz
Dissipation Factor 0.020

@Frequency 8.00e+9 Hz
0.020

@Frequency 8.00e+9 Hz
0.020

@Frequency 1e+10 Hz
0.020

@Frequency 1e+10 Hz
0.020

@Frequency 1.20e+10 Hz
0.020

@Frequency 1.20e+10 Hz
Descriptive Properties Value Comments
Composition MgO+2%SiC