Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.450 - 3.80 W/m-K | 3.12 - 26.4 BTU-in/hr-ft²-°F | Average value: 1.16 W/m-K Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |