Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quantum Composites LYTEX® 4181 55% Carbon Fiber Reinforced Epoxy SMC

Category Polymer , Thermoset , Composite SMC , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Quantum Composites
Trade Name Lytex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quantum Composites LYTEX® 4181 55% Carbon Fiber Reinforced Epoxy SMC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LYTEX 4181 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance and low density. It utilizes a 12K Tow carbon fiber reinforcement.Form = SheetColor = BlackGlass Fiber Content = 55%Information provided by Quantum Composites.
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ASTM D792
Linear Mold Shrinkage 0.00 cm/cm
0.00 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 206 MPa
29900 psi
ASTM D638
Flexural Strength 413 MPa
59900 psi
ASTM D790
Flexural Modulus 31.0 GPa
4500 ksi
ASTM D790
Izod Impact, Notched 8.00 J/cm
15.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Thermal Conductivity 0.450 W/m-K
3.12 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air >= 260 °C
>= 500 °F
Deflection Temperature, Load not specified; ASTM D648
Processing Properties Metric English Comments
Processing Temperature 129 - 166 °C
265 - 330 °F
Mold Temperature
Cure Time 5.00 - 10.0 min
0.0833 - 0.167 hour
Shelf Life 6.00 Month

@Temperature -12.2 °C
6.00 Month

@Temperature 10.0 °F
Descriptive Properties Value Comments
Fiber Length (in) 1
Carbon