Thermal Properties Metric English Comments
CTE, linear 55.0 - 75.0 µm/m-°C
30.6 - 41.7 µin/in-°F
Polykemi
Polykemi AB POLYfill PP EIP12030F Polypropylene/EPDM, Mineral Reinforced
Information provided by Polykemi AB
CTE, linear 55.0 - 75.0 µm/m-°C
30.6 - 41.7 µin/in-°F
Polykemi
Polykemi AB POLYfill PP EIP12030RF Polypropylene/EPDM, Mineral Reinforced
Information provided by Polykemi AB
CTE, linear 59.9 - 75.0 µm/m-°C
33.3 - 41.7 µin/in-°F
Average value: 65.0 µm/m-°C Grade Count:3
Overview of materials for Acrylic, Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o..
CTE, linear 49.0 - 75.0 µm/m-°C

@Temperature 40.0 - 130 °C
27.2 - 41.7 µin/in-°F

@Temperature 104 - 266 °F
Average value: 62.0 µm/m-°C Grade Count:2
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum ..
CTE, linear 72.0 - 75.0 µm/m-°C
40.0 - 41.7 µin/in-°F
Average value: 74.4 µm/m-°C Grade Count:5
Overview of materials for Styrene-Butadiene Copolymer, SBC
This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values ..
CTE, linear 70.0 - 75.0 µm/m-°C
38.9 - 41.7 µin/in-°F
Master Bond MB250NT Low viscosity ethyl cyanoacrylate
Master Bond MB250NT is a single component ethyl cyanoacrylate type system. This rapid curing, high strength system is used primarily in applications where the ISO 10993-5 for low toxicity is specifi..
CTE, linear 70.0 - 75.0 µm/m-°C
38.9 - 41.7 µin/in-°F
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate
Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver..
CTE, linear 74.5 - 75.1 µm/m-°C
41.4 - 41.7 µin/in-°F
Cast Nylons Nycast® SLX Premium Bearing Grade Nylon
Nycast® SLX closes the gap between static and dynamic coefficients of friction. Used in wear pads, bearing blocks, and other load-bearing slide applications.Data provided by the manufacturer, Cast..
CTE, linear 50.0 - 75.0 µm/m-°C
27.8 - 41.7 µin/in-°F
Polykemi
Polykemi AB POLYfill PPH TS5040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
CTE, linear 55.0 - 75.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
30.6 - 41.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL EX130 PPE+HIPS (Asia Pacific)
PPE+PS Auto Exterior Grade