Aptek 2503R-A/B Premeasured conformal urethane coating repair kit

Category Polymer , Adhesive , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive
Manufacturer Aptek Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aptek 2503R-A/B Premeasured conformal urethane coating repair kit.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electrical/electronic components mounted on printed circuit boards. Ideal for repair-ready-to-use; Fully compatible with APTEK 2503-A/B conformal coating as well as other commercially available urethane coatings; Excellent reversion resistance for good physical stability under high heat and humidity environments; Tg below -70ºC for excellent low temperature cycling, storage and performance; Excellent substrate adhesion, superior to silicones; Exceeds NASA outgassing requirements for high vacuum environments; Fluoresces under black-light (UV) to facilitate QC inspection of coating coverage of repaired components/substrates.APTEK 2503R-A is an unfilled polyol resin containing solvent and is thus considered a flammable liquid and should be treated with caution. . APTEK 2503R-B is an organic isocyanate and is safe to handle when used properly. .Information provided by Aptek Laboratories, Inc.
Physical Properties Metric English Comments
Outgassing - Total Mass Loss 0.187 %
0.187 %
Cured property; at 10E-6 torr; ASTM E595
Collected Volatile Condensable Material 0.0020 %
0.0020 %
Cured property; at 10E-6 torr; ASTM E595
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
Cured property; ASTM D2240
Tensile Strength, Ultimate 19.3 MPa
2800 psi
Cured property; ASTM D412
Elongation at Break 525 %
525 %
Cured property; ASTM D412
Thermal Properties Metric English Comments
CTE, linear 180 µm/m-°C

@Temperature 20.0 °C
100 µin/in-°F

@Temperature 68.0 °F
Cured property; alpha 1; JMTP P200
Glass Transition Temp, Tg -74.0 °C
-101 °F
Cured property; JMTP P200
Flash Point 10.0 °C
50.0 °F
A Component; ASTM D92
>= 150 °C
>= 302 °F
B Component; ASTM D92
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Processing Temperature 80.0 °C
176 °F
Cure 8 hrs
100 °C
212 °F
Cure 5 hrs
125 °C
257 °F
Cure 2 hrs