Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP TIVAR® Burnguard PE-UHMW + flame retardant + other additives (ISO Data)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Quadrant Engineering Plastics Products
Trade Name TIVAR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP TIVAR® Burnguard PE-UHMW + flame retardant + other additives (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TIVAR Burnguard is a PE-UHMW grade containing a very effective non-halogenated flame retardant. Specifically developed to improve the poor flammability behaviour of straight forward virgin polyethylene, it meets the requirements of UL 94 V-0 as of 6 mm thickness and is self-extinguishing. The additives used also render this material static dissipative and considerably improve UV-resistance
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ISO 1183-1
Water Absorption <= 0.20 %
<= 0.20 %
96 hr; ISO 62
Moisture Absorption at Equilibrium <= 0.20 %
<= 0.20 %
50% RH
Water Absorption at Saturation <= 0.20 %
<= 0.20 %
ISO 62
Outgassing - Total Mass Loss 0.14 %
0.14 %
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
Ball Indentation Hardness 34.0 MPa
4930 psi
ISO 2039-1
Tensile Strength 16.0 MPa
2320 psi
at Yield; ISO 527-1/-2
Elongation at Break 25 %
25 %
ISO 527-1/-2
Elongation at Yield 15 %
15 %
ISO 527-1/-2
Tensile Modulus 1.00 GPa
145 ksi
ISO 527-1/-2
Flexural Strength 18.0 MPa
2610 psi
Compressive Strength 7.00 MPa

@Strain 1 %
1020 psi

@Strain 1 %
ISO 604
11.0 MPa

@Strain 2 %
1600 psi

@Strain 2 %
ISO 604
17.0 MPa

@Strain 5 %
2470 psi

@Strain 5 %
ISO 604
K Factor (ISO) 14 µm/km
14 µm/km
Charpy Impact Unnotched NB
NB
ISO 179-1/1eU
Charpy Impact, Notched 7.00 J/cm²
33.3 ft-lb/in²
Partial Break; ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.15 - 0.30
0.15 - 0.30
Sand Slurry 130
130
Limiting Pressure Velocity 0.0500 MPa-m/sec
1430 psi-ft/min
at 1 m/s unlubricated
0.0800 MPa-m/sec
2280 psi-ft/min
at 0.1 m/s unlubricated
Thermal Properties Metric English Comments
CTE, linear 180 µm/m-°C

@Temperature 23.0 - 100 °C
100 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.400 W/m-K
2.78 BTU-in/hr-ft²-°F
Melting Point 135 °C
275 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C
108 °F
ISO 75-1/-2
Flammability, UL94 V-0
V-0
Oxygen Index 28 %
28 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 1e+05
<= 1e+05
IEC 60093
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Acceptable
Acceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Acceptable
Acceptable
Conductive / Static Dissipative Yes
Yes
Continuous Sunlight Limited
Limited
Hot Water / Steam Unacceptable
Unacceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Limited
Limited
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Copyright © lookpolymers.com All Rights Reserved