CPC - Vycom HITEC® Pipe Grade HDPE High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer CPC - Vycom Co.
Trade Name HITEC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CPC - Vycom HITEC® Pipe Grade HDPE High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hitec pipe grade HDPE is a special formulation that has high impact strength, and environmental stress crack resistance. Hitec Pipe grade meets Federal specification L-P 390C, ASTM D1248 Type III weather resistant black and ASTM 3350 cell class 345464C.FEATURES AND BENEFITS Hardness- Hitec Pipe Grade is abrasion resistant and will resist scratching. Strength- Hitec Pipe Grade has high tensile and stiffness for machine parts and tank applications. Ductility- Hitec Pipe Grade is stress crack resistant. Machinable- Hitec Pipe Grade is easy to machine with conventional tools.Information provided by Compression Polymers Corp - Vycom
Physical Properties Metric English Comments
Density 0.957 g/cc
0.0346 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 1000 hour

@Temperature >=50.0 °C
>= 1000 hour

@Temperature >=122 °F
Igepal (no failures); ASTM F1248
ESCR 100% Igepal® >= 5000 hour
>= 5000 hour
no failures; ASTM D 1693C
Mechanical Properties Metric English Comments
Hardness, Rockwell L 49
49
ASTM D785
Hardness, Shore D 63
63
ASTM D2240
Tensile Strength, Ultimate >= 22.8 MPa

@Thickness 3.17 mm
>= 3300 psi

@Thickness 0.125 in
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.862 GPa
125 ksi
at 2% Strain; ASTM D3350
2% Secant Modulus 0.793 GPa
115 ksi
ASTM D638
Izod Impact, Notched 4.27 J/cm
8.00 ft-lb/in
ASTM D 256A
Hydrostatic Design Basis 11.0 MPa
1600 psi
100,000 hrs.; ASTM D2837
Thermal Properties Metric English Comments
CTE, linear 180 µm/m-°C

@Temperature 20.0 °C
100 µin/in-°F

@Temperature 68.0 °F
ASTM D648
Melting Point 127 °C
260 °F
ASTM D3417
Vicat Softening Point 124 °C
255 °F
ASTM D1525
Brittleness Temperature -118 °C
-180 °F
ASTM D746