Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 16.0 µm/m-°C | 8.89 µin/in-°F | X-Direction; TMA; 10°C/min; ASTM D3386; IPC-TM-650 2.4.41 |
Rogers Corporation RT/duroid® 6002 High Frequency Laminate Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric.. |
|||
CTE, linear | 16.0 µm/m-°C | 8.89 µin/in-°F | Y-Direction; TMA; 10°C/min; ASTM D3386; IPC-TM-650 2.4.41 |
Rogers Corporation RT/duroid® 6002 High Frequency Laminate Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric.. |
|||
CTE, linear | 16.0 µm/m-°C | 8.89 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI)
(Unverified Data**) Torlon 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics simil.. |
|||
CTE, linear | 16.0 - 85.5 µm/m-°C | 8.89 - 47.5 µin/in-°F | Average value: 50.8 µm/m-°C Grade Count:37 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
CTE, linear | 16.0 µm/m-°C | 8.89 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105-7442 PEEK, with carbon fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi.. |
|||
CTE, linear | 16.0 µm/m-°C @Temperature 20.0 °C |
8.89 µin/in-°F @Temperature 68.0 °F |
|
Indium Corp. Indalloy® 182 Au-Sn Solder Alloy Eutectic die attach and package sealing.Information provided by the manufacturer, Indium Corporation. |
|||
CTE, linear | 16.0 µm/m-°C @Temperature 21.1 - 102 °C |
8.90 µin/in-°F @Temperature 70.0 - 215 °F |
|
Materion ToughMet® T3 AT110 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
CTE, linear | 16.0 µm/m-°C @Temperature 21.1 - 102 °C |
8.90 µin/in-°F @Temperature 70.0 - 215 °F |
|
Materion ToughMet® T3 AT120 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
CTE, linear | 16.0 µm/m-°C @Temperature 21.1 - 102 °C |
8.90 µin/in-°F @Temperature 70.0 - 215 °F |
|
Materion ToughMet® T3 AT90 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
CTE, linear | 16.0 µm/m-°C @Temperature 20.0 °C |
8.89 µin/in-°F @Temperature 68.0 °F |
x-axis |
Industrial Laminates/Norplex NP631 Paper Base Laminate Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500" |
|||
CTE, linear | 16.0 µm/m-°C @Temperature 20.0 °C |
8.90 µin/in-°F @Temperature 68.0 °F |
|
SGL Carbon Group Ridurid® V 1640 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
CTE, linear | 16.0 - 17.1 µm/m-°C @Temperature 25.0 - 300 °C |
8.89 - 9.50 µin/in-°F @Temperature 77.0 - 572 °F |
|
Goodfellow Awa®, Nickeloid®, Simlet®, Spedex® Nickel Silver Good machinability, excellent cold working and welding characteristics. Poor hot forming. Uses include rivets, screws, zippers, optical parts and costume jewelry.Information provided by Goodfello.. |
|||
CTE, linear | 16.0 µm/m-°C | 8.89 µin/in-°F | |
Hexcel® HexPly® F263 Epoxy Resin HexPly® F263 is a structural, heat resistant epoxy resin formulated for excellent translation of high modulus carbon fiber properties in typically aerospace applications. HexPly® F263 is a high te.. |
|||
CTE, linear | 16.0 µm/m-°C | 8.89 µin/in-°F | Absolute Drying; ASTM-D696 |
Toyobo GLAMIDE® TY-592GHV 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
CTE, linear | 16.0 µm/m-°C @Temperature 20.0 - 649 °C |
8.90 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Eagle Brass 200/201 Nickel Alloy, 1/4 Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
CTE, linear | 16.0 µm/m-°C @Temperature 20.0 - 649 °C |
8.90 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Eagle Brass 200/201 Nickel Alloy, 3/4 Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
CTE, linear | 16.0 µm/m-°C @Temperature 20.0 - 649 °C |
8.90 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Eagle Brass 200/201 Nickel Alloy, Full Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
CTE, linear | 16.0 µm/m-°C @Temperature 0.000 - 100 °C |
8.89 µin/in-°F @Temperature 32.0 - 212 °F |
|
CLAL-MSX NICLAL 1800 0 Annealed Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good corrosion resistanceHigh mechanical propertiesTypical Applications:Parts subject to high stressHigh quality fastenersInformation provided by CLAL-MSX |
|||
CTE, linear | 16.0 µm/m-°C @Temperature 0.000 - 100 °C |
8.89 µin/in-°F @Temperature 32.0 - 212 °F |
|
CLAL-MSX NICLAL 1800 H12 1/2 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good corrosion resistanceHigh mechanical propertiesTypical Applications:Parts subject to high stressHigh quality fastenersInformation provided by CLAL-MSX |
|||
CTE, linear | 16.0 µm/m-°C @Temperature 0.000 - 100 °C |
8.89 µin/in-°F @Temperature 32.0 - 212 °F |
|
CLAL-MSX NICLAL 1300 H14 4/4 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX |
|||
CTE, linear | 16.0 µm/m-°C @Temperature 50.0 - 150 °C |
8.89 µin/in-°F @Temperature 122 - 302 °F |
IPC TM-650 2.4.41 |
Arlon AD250C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.50) with Tight Tolerance.. |
|||
CTE, linear | 16.0 µm/m-°C | 8.89 µin/in-°F | x direction |
Arlon AD255A Glass, PTFE and Micro-Dispersed Ceramic Lower Loss and Improved Performance over Traditional AD Series.Information provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear | 16.0 µm/m-°C @Temperature 50.0 - 150 °C |
8.89 µin/in-°F @Temperature 122 - 302 °F |
IPC TM-650 2.4.41 |
Arlon AD255C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.55) with Tighter Toleran.. |
|||
CTE, linear | 16.0 - 500 µm/m-°C | 8.89 - 278 µin/in-°F | Average value: 183 µm/m-°C Grade Count:12 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
CTE, linear | 16.0 µm/m-°C @Temperature 21.1 - 102 °C |
8.90 µin/in-°F @Temperature 70.0 - 215 °F |
|
Materion ToughMet® T3 AT90 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |